Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Cast Nylons Nycast® GX Solid Lubricant Filled Gray Cast Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Cast
Manufacturer Cast Nylons Limited
Trade Name Nycast®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cast Nylons Nycast® GX Solid Lubricant Filled Gray Cast Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
NYCAST® GX is a specially formulated, self-lubricating grade designed to deliver low coefficient of friction, superior wear resistance, high pressure/velocity performance, and low moisture absorption. Typical applications include wear pads, bearings, thrust washers, bushings, and gears.Data provided by the manufacturer, Cast Nylons Limited.
Physical Properties Metric English Comments
Density 1.14 - 1.15 g/cc
0.0412 - 0.0415 lb/in³
ASTM D792
Water Absorption 0.40 - 0.50 %
0.40 - 0.50 %
24 hrs; ASTM D570
Water Absorption at Saturation 4.0 - 5.0 %
4.0 - 5.0 %
ASTM D570
Deformation 0.70 - 0.80 %
0.70 - 0.80 %
ASTM D621
Mechanical Properties Metric English Comments
Hardness, Rockwell R 103
103
ASTM D785
Hardness, Shore D 78
78
ASTM D2240
Tensile Strength 65.5 - 75.8 MPa
9500 - 11000 psi
ASTM D638
Elongation at Break 45 - 50 %
45 - 50 %
ASTM D638
Tensile Modulus 2.59 - 3.28 GPa
375 - 475 ksi
ASTM D638
Flexural Strength 96.5 - 110 MPa
14000 - 16000 psi
ASTM D790
Flexural Modulus 2.59 - 3.28 GPa
375 - 475 ksi
ASTM D790
Compressive Strength 82.7 - 96.5 MPa
12000 - 14000 psi
ASTM D695
Compressive Modulus 1.90 - 2.59 GPa
275 - 375 ksi
ASTM D695
Shear Strength 55.2 - 62.1 MPa
8000 - 9000 psi
ASTM D732
Izod Impact, Notched 0.747 - 0.961 J/cm
1.40 - 1.80 ft-lb/in
ASTM D256
Coefficient of Friction, Dynamic 0.12
0.12
ASTM D1894
Coefficient of Friction, Static 0.25 - 0.35
0.25 - 0.35
ASTM D1894
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C
50.0 µin/in-°F
Melting Point 227 - 238 °C
440 - 460 °F
Maximum Service Temperature, Air 110 °C
230 °F
Continuous
166 °C
330 °F
Intermittent
Deflection Temperature at 0.46 MPa (66 psi) 212 °C
413 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 81.7 °C
179 °F
ASTM D648
Electrical Properties Metric English Comments
Dielectric Constant 3.7

@Frequency 60.0 Hz
3.7

@Frequency 60.0 Hz
ASTM D150
3.7

@Frequency 1000 Hz
3.7

@Frequency 1000 Hz
ASTM D150
3.7

@Frequency 1.00e+6 Hz
3.7

@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 19.7 - 23.6 kV/mm
500 - 600 kV/in
ASTM D149