Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Lubri-Tech™ ES-20GF/08T Polyethersulfone - 20% Glass Fiber And PTFE  (discontinued **)

Category Polymer , Thermoplastic , Polyethersulfone (PES)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Lubri-Tech™ ES-20GF/08T Polyethersulfone - 20% Glass Fiber And PTFE  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by PolyOne.
Physical Properties Metric English Comments
Density 1.56 g/cc
0.0564 lb/in³
ASTM D792
Water Absorption 0.20 %
0.20 %
24 hrs. ASTM D570
Linear Mold Shrinkage 0.0030 cm/cm

@Thickness 3.17 mm
0.0030 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 121 MPa
17500 psi
ASTM D638
Elongation at Break 2.0 - 4.0 %
2.0 - 4.0 %
ASTM D638
Tensile Modulus 5.50 GPa
798 ksi
ASTM D638
Flexural Yield Strength 165 MPa
23900 psi
ASTM D790
Flexural Modulus 5.50 GPa
798 ksi
ASTM D790
Izod Impact, Notched 0.690 - 0.960 J/cm

@Thickness 6.35 mm
1.29 - 1.80 ft-lb/in

@Thickness 0.250 in
ASTM D256
Processing Properties Metric English Comments
Melt Temperature 354 - 382 °C
669 - 720 °F
Stock
Mold Temperature 121 - 149 °C
250 - 300 °F
Drying Temperature 121 - 149 °C
250 - 300 °F