Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.640 - 0.960 J/cm @Thickness 6.35 mm |
1.20 - 1.80 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
PolyOne Edgetek® ES-20GF-15GM/000 Polyethersulfone - 20% Glass Fiber - 15% Milled Glass
(discontinued **) Data provided by PolyOne. |
|||
Izod Impact, Notched | 0.400 - 0.960 J/cm @Temperature -40.0 - -29.0 °C |
0.749 - 1.80 ft-lb/in @Temperature -40.0 - -20.2 °F |
Average value: 0.620 J/cm Grade Count:3 |
Overview of materials for Acetal Homopolymer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced". Each property range of values reported is minimum and maximum values .. |
|||
Izod Impact, Notched | 0.750 - 0.960 J/cm | 1.41 - 1.80 ft-lb/in | Average value: 0.873 J/cm Grade Count:3 |
Overview of materials for Glass Reinforced, Modified SMA This property data is a summary of similar materials in the MatWeb database for the category "Glass Reinforced, Modified SMA". Each property range of values reported is minimum and maximum values of.. |
|||
Izod Impact, Notched | 0.690 - 0.960 J/cm @Thickness 6.35 mm |
1.29 - 1.80 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
PolyOne Lubri-Tech™ NL-10GF/15TF Nylon 6/12 - 10% Glass Fiber - 15% PTFE Flock
(discontinued **) Data provided by PolyOne. |
|||
Izod Impact, Notched | 0.690 - 0.960 J/cm @Thickness 6.35 mm |
1.29 - 1.80 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
PolyOne Lubri-Tech™ ES-20GF/08T Polyethersulfone - 20% Glass Fiber And PTFE
(discontinued **) Data provided by PolyOne. |
|||
Izod Impact, Notched | 0.590 - 0.960 J/cm @Thickness 6.35 mm |
1.11 - 1.80 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
PolyOne Lubri-Tech™ MP-000/10T Modified PPO - 10% PTFE
(discontinued **) Data provided by PolyOne. |