Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.402 - 1.23 J/cm | 0.753 - 2.30 ft-lb/in | Average value: 0.681 J/cm Grade Count:45 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Izod Impact, Notched | 0.690 - 1.23 J/cm @Temperature -40.0 - -40.0 °C |
1.29 - 2.30 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 1.01 J/cm Grade Count:45 |
Overview of materials for Cellulose Acetate Propionate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate Propionate, Molded". Each property range of values reported is minimum and maximum val.. |
|||
Izod Impact, Notched | 0.370 - 1.23 J/cm @Temperature -40.0 - -40.0 °C |
0.693 - 2.30 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 0.991 J/cm Grade Count:38 |
Overview of materials for Cellulose Acetate Butyrate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate Butyrate, Molded". Each property range of values reported is minimum and maximum value.. |
|||
Izod Impact, Notched | 0.267 - 1.23 J/cm | 0.500 - 2.30 ft-lb/in | Average value: 0.432 J/cm Grade Count:11 |
Overview of materials for Polyphthalamide (PPA), 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are .. |
|||
Izod Impact, Notched | 0.641 - 1.23 J/cm | 1.20 - 2.30 ft-lb/in | Average value: 0.894 J/cm Grade Count:8 |
Overview of materials for Polystyrene + Polyphenylene Ether, Glass Filler This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Glass Filler". Each property range of values reported is minimum and .. |
|||
Izod Impact, Notched | 0.320 - 1.23 J/cm | 0.600 - 2.30 ft-lb/in | Average value: 0.776 J/cm Grade Count:11 |
Overview of materials for Acrylic, Gamma Radiation Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Gamma Radiation Resistant, Molded". Each property range of values reported is minimum and maxim.. |