Material Notes:
REPOL Polypropylene B250EG is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific catalyst system. Repol B250EG is recommended for use in extrusion coating process where high flow is required. It is an ideal material for coating of polypropylene woven fabrics. Features:Excellent flow characteristicsConsistent processabilityGood surface finish and glossInformation provided by Reliance Industries
Physical Properties Metric English Comments
Melt Flow 25 g/10 min

@Load 2.16 kg,
Temperature 230 °C
25 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.0 MPa
3480 psi
50mm/min; ASTM D638
Elongation at Yield 6.0 %
6.0 %
50mm/min; ASTM D638
Flexural Modulus 0.900 GPa
131 ksi
1% secant; ASTM D790A
Izod Impact, Notched 0.500 J/cm

@Temperature 23.0 °C
0.937 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C
203 °F
ASTM D648