Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.450 - 3.00 J/cm @Temperature -17.8 - 0.000 °C |
0.843 - 5.62 ft-lb/in @Temperature 0.000 - 32.0 °F |
Average value: 1.28 J/cm Grade Count:11 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and .. |
|||
Izod Impact, Notched | 0.350 - 3.00 J/cm @Temperature -50.0 - 0.000 °C |
0.656 - 5.62 ft-lb/in @Temperature -58.0 - 32.0 °F |
Average value: 0.922 J/cm Grade Count:13 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Molded". Each property range of values reported is minimum and ma.. |
|||
Izod Impact, Notched | 0.500 - 3.00 J/cm @Temperature -20.0 - 0.000 °C |
0.937 - 5.62 ft-lb/in @Temperature -4.00 - 32.0 °F |
Average value: 1.14 J/cm Grade Count:4 |
Overview of materials for Polypropylene, Sheet/Thermoforming Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Sheet/Thermoforming Grade". Each property range of values reported is minimum and maximum.. |
|||
Izod Impact, Notched | 0.500 - 3.00 J/cm @Thickness 3.20 - 3.20 mm |
0.937 - 5.62 ft-lb/in @Thickness 0.126 - 0.126 in |
Average value: 1.14 J/cm Grade Count:4 |
Overview of materials for Polypropylene, Sheet/Thermoforming Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Sheet/Thermoforming Grade". Each property range of values reported is minimum and maximum.. |