Polymer Property : Izod Impact, Notched = 3.00 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.450 - 3.00 J/cm

@Temperature -17.8 - 0.000 °C
0.843 - 5.62 ft-lb/in

@Temperature 0.000 - 32.0 °F
Average value: 1.28 J/cm Grade Count:11
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and ..
Izod Impact, Notched 0.350 - 3.00 J/cm

@Temperature -50.0 - 0.000 °C
0.656 - 5.62 ft-lb/in

@Temperature -58.0 - 32.0 °F
Average value: 0.922 J/cm Grade Count:13
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Molded". Each property range of values reported is minimum and ma..
Izod Impact, Notched 0.500 - 3.00 J/cm

@Temperature -20.0 - 0.000 °C
0.937 - 5.62 ft-lb/in

@Temperature -4.00 - 32.0 °F
Average value: 1.14 J/cm Grade Count:4
Overview of materials for Polypropylene, Sheet/Thermoforming Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Sheet/Thermoforming Grade". Each property range of values reported is minimum and maximum..
Izod Impact, Notched 0.500 - 3.00 J/cm

@Thickness 3.20 - 3.20 mm
0.937 - 5.62 ft-lb/in

@Thickness 0.126 - 0.126 in
Average value: 1.14 J/cm Grade Count:4
Overview of materials for Polypropylene, Sheet/Thermoforming Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Sheet/Thermoforming Grade". Each property range of values reported is minimum and maximum..