Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 105 MPa | 15200 psi | ISO 2039-1 |
Nilit FRIANYL B63 BR90 Nylon 6.6 for injection molding, 90% bronze filled Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 105 - 230 MPa | 15200 - 33400 psi | Average value: 185 MPa Grade Count:11 |
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled". Specific grades with glass content between 25.. |
|||
Ball Indentation Hardness | 105 MPa | 15200 psi | DIN 53456 |
Ineos Nova S-3222 Medium Impact Compact Polystyrene
(discontinued **) All mechanical properties measured under standard conditions 50% RH and 23°C.Information provided by NOVA Chemicals.INEOS NOVA began October 1 2007 as an expansion of the 50:50 joint venture betwee.. |
|||
Ball Indentation Hardness | 105 MPa | 15200 psi | DIN 53456 |
Global PP-1111-R Polypropylene Homopolymer Description-transparency, high stiffness, high heat resistantApplications-electrical/electronic Information provided by Global Polymers Corporation. |
|||
Ball Indentation Hardness | 105 MPa | 15200 psi | ISO 2039 |
GEHR Plastics ECOGEHR® PLA-LF Polylactic Acid PLA-L is a blend of polylactide, lignin, lingo-cellulosic, natural fatty acids, waxes and wood fibers. This material possesses good mechanical properties similar to ABS. This bioplastic has an opera.. |
|||
Ball Indentation Hardness | 105 MPa | 15200 psi | ISO 2039-1 |
Ineos ABS Lustran® ABS E211 LNS013 Pellets (a-methylstyrene-SAN-modified), Extrusion Grade Lustran® ABS E211 LNS013 is extrusion grade with high heat resistance. It is used for the production of molded plastic articles. |
|||
Ball Indentation Hardness | 105 MPa | 15200 psi | ISO 2039-1 |
Styrolution Novodur® E211 ABS Novodur E211 is a high heat extrusion grade and suitable for blow moldingInformation provided by Styrolution |
|||
Ball Indentation Hardness | 105 MPa | 15200 psi | ISO 2039-1 |
Styrolution Novodur® H604 ABS Novodur H604 is a high heat injection molding grade with enhanced chemical resistance, especially suitable for being painted.Information provided by Styrolution |
|||
Ball Indentation Hardness | 105 MPa | 15200 psi | ISO 2039-1 |
Styrolution Novodur® H605 ABS Novodur H605 is a high heat injection molding grade with enhanced flowability and reduced emission.Information provided by Styrolution |
|||
Ball Indentation Hardness | 105 MPa | 15200 psi | ISO 2039-1 |
Styrolution Novodur® H702 ABS Novodur H702 is a high heat, high gloss injection molding grade with very good flowabilityInformation provided by Styrolution |
|||
Ball Indentation Hardness | 105 MPa | 15200 psi | ISO 2039-1 |
Styrolution Novodur® M201AS ABS Novodur M201AS is a medium impact, high gloss injection molding grade with improved chemical resistanceInformation provided by Styrolution |
|||
Ball Indentation Hardness | 105 MPa | 15200 psi | ISO 2039-1 |
Styrolution Novodur® M203FC ABS Novodur HD M203FC is an injection molding grade especially suitable for medical applications providing high flowability.Information provided by Styrolution |
|||
Ball Indentation Hardness | 105 MPa | 15200 psi | DIN 53459 |
Styron Pulse® A35-105 PC/ABS PULSE™ A35-105 engineering resins give exceptional impact strength even at low temperatures and have high heat distortion temperature.Information provided by DowThis product line was spun off f.. |
|||
Ball Indentation Hardness | 105 MPa | 15200 psi | DIN 53459 |
Styron Pulse® A35-110 PC/ABS PULSE™ A35-110 engineering resins give exceptional impact strength even at low temperatures and have high heat distortion temperature. The proprietary mass ABS technology of Dow allows these p.. |
|||
Ball Indentation Hardness | 105 MPa | 15200 psi | ISO 2039-1 |
Styrolution Novodur® H801 ABS / PC Novodur H801 is a high heat injection molding grade with high impact strength and reduced emission.Information provided by Styrolution |
|||
Ball Indentation Hardness | 105 MPa | 15200 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® EBGM-30 HX PA666-GF30 Product description: Grilon EBGM-30 HX is a specially heat stabilized PA66+PA6 injection molding grade with 30% glass fibers. Grilon EBGM-30 HX has the following important properties: High heat resi.. |
|||
Ball Indentation Hardness | 105 MPa | 15200 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® XE 4129 black 9020 PA610 Product description: Grilamid XE 4129 black 9020 is a high viscosity Polyamide 610 especially suitable for extrusion applications. A characteristic of tubes made out of this material is the high res.. |
|||
Ball Indentation Hardness | 105 MPa @Load 36.5 kg, Time 30.0 sec |
15200 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
BASF Ultraform® N2640 E2 POM Description: Is a POM + MBS, elastomer-modified injection-molding grade with enhanced toughness and high weld line strength.Information provided by BASF |
|||
Ball Indentation Hardness | 105 MPa | 15200 psi | ISO 2039-1 |
CENTROPLAST BC NF Organic Thermoplastic, 15% Natural Fiber CENTROPLAST BC NF 15 is made of CO2-neutral, sustainable raw-materials with 15% natural fiber.CENTROPLAST has the characteristics of thermoplastics while being 100% recyclable and completely biodegr.. |
|||
Ball Indentation Hardness | 105 - 125 MPa | 15200 - 18100 psi | ISO 2032-N132 |
Adamas Adalon® 704 PTFE, Long Carbon Fiber Information provided by Adamas, HPM |
|||
Ball Indentation Hardness | 105 MPa @Load 36.5 kg, Time 30.0 sec |
15200 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
BASF Ultraform® N2650 Z2 (LEV) POM Description: Is a POM + PUR, elastomer-modified injection-molding grades with high impact strength for clips, snap and fastening elements, also for components subject to impact stress.Information pr.. |
|||
Ball Indentation Hardness | 105 MPa @Time 30.0 sec |
15200 psi @Time 0.00833 hour |
DIN 53 456 |
Hippe PVDF Better mechanical strength compared to other fluorinated polymers. Tough and hard. High-grade electrical feature. Good weathering stability. Physiologically safe. Not as good as fluorinated pol.. |
|||
Ball Indentation Hardness | 105 MPa | 15200 psi | ISO 2039-1 |
BASF Ultradur® B 4300 M2 12.5% Mineral Filled PBT Description: Is a PBT-HI, mineral-reinforced, impact-modified injection-molding grade for rigid parts, for example automotive power door locks.Information provided by BASF |
|||
Ball Indentation Hardness | 105 MPa | 15200 psi | ISO 2039-1 |
CENTROPLAST BC Organic Thermoplastic CENTROPLAST BC is made of CO2-neutral, sustainable raw-materials.CENTROPLAST has the characteristics of thermoplastics while being 100% recyclable and completely biodegradable by composting accordin.. |