Material Notes:
Better mechanical strength compared to other fluorinated polymers. Tough and hard. High-grade electrical feature. Good weathering stability. Physiologically safe. Not as good as fluorinated polymers in terms of dielectricity.Information provided by Hippe.
Physical Properties Metric English Comments
Specific Gravity 1.79 g/cc
1.79 g/cc
DIN 53 479
Moisture Absorption at Equilibrium <= 0.050 %
<= 0.050 %
Absorption of humidity in standard operating environment; DIN 53 715
Water Absorption at Saturation <= 0.050 %
<= 0.050 %
DIN 53 495
Mechanical Properties Metric English Comments
Ball Indentation Hardness 105 MPa

@Time 30.0 sec
15200 psi

@Time 0.00833 hour
DIN 53 456
Tensile Strength 55.0 MPa
7980 psi
DIN 53 455
Elongation at Break 20 - 400 %
20 - 400 %
DIN 53 455
Tensile Modulus 2.00 GPa
290 ksi
DIN 53 457
Flexural Modulus 2.00 GPa
290 ksi
from bending test; DIN 53 457
Charpy Impact, Notched NB
NB
DIN 53 453
Coefficient of Friction, Dynamic 0.30
0.30
Against steel, p=0.05 N/mm², v=0.6 m/s, hardened and ground
Thermal Properties Metric English Comments
CTE, linear 130 µm/m-°C
72.2 µin/in-°F
Specific Heat Capacity 1.20 J/g-°C
0.287 BTU/lb-°F
Thermal Conductivity 0.110 W/m-K
0.763 BTU-in/hr-ft²-°F
Melting Point 178 °C
352 °F
DIN 53 736
Maximum Service Temperature, Air 150 °C
302 °F
Continuous use
150 °C
302 °F
Short Periods
Deflection Temperature at 0.46 MPa (66 psi) 140 °C
284 °F
ISO-R 75 Method B
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C
203 °F
ISO-R 75 Method A
Glass Transition Temp, Tg -18.0 °C
-0.400 °F
dynamic; DIN 53 736
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 4.00e+14 ohm-cm
4.00e+14 ohm-cm
DIN 53 482, VDE 0303, Part 3
Surface Resistance >= 1.00e+13 ohm
>= 1.00e+13 ohm
DIN 53 482
Dielectric Constant 8.0

@Frequency 1.00e+6 Hz
8.0

@Frequency 1.00e+6 Hz
DIN 53 483, IEC-250
Dielectric Strength 17.0 - 150 kV/mm
432 - 3810 kV/in
Breakdown; DIN 53 481, IEC-243, VDE 0303 Part 1
Dielectric Loss Index 0.060

@Frequency 1.00e+6 Hz
0.060

@Frequency 1.00e+6 Hz
DIN 53 483, IEC-250
Descriptive Properties Value Comments
Color white
Creep Resistance Grade CTI 600
DIN 53 480, IEC-112, VDE 0303 Part 1
Resistance to hot water, suds resistant