EMS-Grivory Grivory® EBGM-30 HX PA666-GF30

Category Polymer , Thermoplastic , Nylon , Nylon 6/66 , Nylon 66/6, 30% Glass Fiber Reinforced
Manufacturer EMS-Grivory (EMS-CHEMIE)
Trade Name Grivory®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Grivory Grivory® EBGM-30 HX PA666-GF30.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product description: Grilon EBGM-30 HX is a specially heat stabilized PA66+PA6 injection molding grade with 30% glass fibers. Grilon EBGM-30 HX has the following important properties: High heat resistanceHigh stiffnessGood flowabilityGood welding behavior Application examples: Grilon EBGM-30 HZ is especially suitable for production of technical parts in the application fields of:Charged air ductsConnectors for air ductsApplications under the bonnetAll applications with high heat resistance.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.37 g/cc
0.0495 lb/in³
ISO 1183
Water Absorption 5.5 %
5.5 %
ISO 62
Moisture Absorption 2.00 %
2.00 %
ISO 62
Linear Mold Shrinkage, Flow 0.0020 cm/cm
0.0020 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
0.0080 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Ball Indentation Hardness 105 MPa
15200 psi
conditioned; ISO 2039-1
210 MPa
30500 psi
dry; ISO 2039-1
Tensile Strength at Break 90.0 MPa
13100 psi
conditioned; ISO 527-1/-2
155 MPa
22500 psi
dry; ISO 527-1/-2
Elongation at Break 3.0 %
3.0 %
dry; ISO 527-1/-2
6.0 %
6.0 %
conditioned; ISO 527-1/-2
Tensile Modulus 5.50 GPa
798 ksi
conditioned; ISO 527-1/-2
9.50 GPa
1380 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched 7.00 J/cm²
33.3 ft-lb/in²
dry; ISO 179/1eU
7.00 J/cm²
33.3 ft-lb/in²
conditioned; ISO 179/1eU
6.50 J/cm²

@Temperature 30.0 °C
30.9 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
6.50 J/cm²

@Temperature 30.0 °C
30.9 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 1.00 J/cm²
4.76 ft-lb/in²
dry; ISO 179/1eA
1.10 J/cm²
5.23 ft-lb/in²
conditioned; ISO 179/1eA
0.700 J/cm²

@Temperature 30.0 °C
3.33 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
0.700 J/cm²

@Temperature 30.0 °C
3.33 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 20.0 µm/m-°C
11.1 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 80.0 µm/m-°C
44.4 µin/in-°F
ISO 11359-1/-2
Melting Point 260 °C
500 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 130 - 150 °C
266 - 302 °F
long term; EMS
230 °C
446 °F
short term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 225 °C
437 °F
ISO 75-1/-2
Deflection Temperature at 8.0 MPa 155 °C
311 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
conditioned; IEC 60093
1.00e+12 ohm-cm
1.00e+12 ohm-cm
dry; IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Strength 34.0 kV/mm
864 kV/in
conditioned; IEC 60243-1
38.0 kV/mm
965 kV/in
dry; IEC 60243-1
Comparative Tracking Index 500 V
500 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Automotive Air intake sytems
Form Granules
Processing Extrusion - blow molding
Injection Molding
Other Extrusion
Product Attributes Nanocomposite
Special Characteristics Improved heat resistance