Mechanical Properties Metric English Comments
Ball Indentation Hardness 105 - 230 MPa
15200 - 33400 psi
Average value: 185 MPa Grade Count:11
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled". Specific grades with glass content between 25..
Ball Indentation Hardness 90.0 - 230 MPa
13100 - 33400 psi
Average value: 192 MPa Grade Count:8
Overview of materials for Polyetheretherketone, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Unreinforced". Each property range of values reported is minimum and maximum value..
Ball Indentation Hardness 20.0 - 230 MPa
2900 - 33400 psi
Average value: 122 MPa Grade Count:59
Overview of materials for Nylon 12
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12". Each property range of values reported is minimum and maximum values of appropriate MatWeb en..
Ball Indentation Hardness 155 - 230 MPa
22500 - 33400 psi
Average value: 189 MPa Grade Count:16
Overview of materials for Nylon 12, 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. ..
Ball Indentation Hardness 70.0 - 230 MPa
10200 - 33400 psi
Average value: 169 MPa Grade Count:52
Overview of materials for Nylon 6, 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. E..