Adamas Adalon® 704 PTFE, Long Carbon Fiber

Category Polymer , Thermoplastic , Fluoropolymer , PTFE
Manufacturer Adamas
Trade Name Adalon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Adamas Adalon® 704 PTFE, Long Carbon Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Adamas, HPM
Physical Properties Metric English Comments
Specific Gravity 1.89 - 1.91 g/cc
1.89 - 1.91 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 64 - 68
64 - 68
ASTM D2240
Ball Indentation Hardness 105 - 125 MPa
15200 - 18100 psi
ISO 2032-N132
Tensile Strength at Break >= 18.0 MPa
>= 2610 psi
ASTM D4745-11
Elongation at Break >= 20 %
>= 20 %
ASTM D4745-11
Thermal Properties Metric English Comments
Thermal Conductivity 0.380 W/m-K
2.64 BTU-in/hr-ft²-°F
ASTM C 177
Melting Point 327 °C
621 °F
DSC
Maximum Service Temperature, Air 260 °C
500 °F
DSC
Minimum Service Temperature, Air -140 °C
-220 °F
DSC
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 10000 ohm-cm
10000 ohm-cm
ASTM D257
Surface Resistance 1000 ohm
1000 ohm
ASTM D257