DSM Arnitel® CM600-V TPC-ES FR

Category Polymer , Thermoplastic , Elastomer, TPE , Polyester TPE , Polyester, TP
Manufacturer DSM Engineering Plastics
Trade Name Arnitel®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Arnitel® CM600-V TPC-ES FR.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Extrusion, Flame Retardant (Halogen free)
Physical Properties Metric English Comments
Density 1.32 g/cc
0.0477 lb/in³
ISO 1183
Melt Flow 13 g/10 min

@Load 2.16 kg,
Temperature 230 °C
13 g/10 min

@Load 4.76 lb,
Temperature 446 °F
cm<sup>3</sup>/10min Melt Volume-flow Rate; ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 61

@Time 3.00 sec
61

@Time 0.000833 hour
ISO 868
Tensile Strength, Ultimate 20.5 MPa
2970 psi
ISO 527-1/-2
Tensile Stress 16.0 MPa

@Strain 5.00 %
2320 psi

@Strain 5.00 %
ISO 527-1/-2
16.0 MPa

@Strain 100 %
2320 psi

@Strain 100 %
ISO 527-1/-2
17.5 MPa

@Strain 50.0 %
2540 psi

@Strain 50.0 %
ISO 527-1/-2
19.5 MPa

@Strain 10.0 %
2830 psi

@Strain 10.0 %
ISO 527-1/-2
Elongation at Break 200 %
200 %
ISO 527-1/-2
Tensile Modulus 0.420 GPa
60.9 ksi
ISO 527-1/-2
Izod Impact Resistance NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 180/1A
Charpy Impact, Notched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 205 °C
401 °F
10°C/min; ISO 11357-1/-3
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
IEC 60093
Dielectric Constant 3.7

@Frequency 1.00e+6 Hz
3.7

@Frequency 1.00e+6 Hz
IEC 60250
4.2

@Frequency 100 Hz
4.2

@Frequency 100 Hz
IEC 60250
Dielectric Strength 18.7 kV/mm
475 kV/in
IEC 60243-1
Dissipation Factor 0.0157

@Frequency 100 Hz
0.0157

@Frequency 100 Hz
IEC 60250
0.0385

@Frequency 1.00e+6 Hz
0.0385

@Frequency 1.00e+6 Hz
IEC 60250