DuPont Performance Polymers Hytrel® G5564 TPC-ET  (Unverified Data**)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyester, TP , Polyester Thermoplastic Elastomer
Manufacturer DuPont Performance Polymers
Trade Name Hytrel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Hytrel® G5564 TPC-ET  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hytrel® G5564 is a 55 nom. Shore D, heat stable, plasticiser free high viscosity resin for extrusion; low temperature impact resistance as well as excellent mechanical properties; good hydrocarbon resistance.Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.21 g/cc
0.0437 lb/in³
ISO 1183
Water Absorption 0.50 %

@Temperature 23.0 °C
0.50 %

@Temperature 73.4 °F
Equilibrium 50%RH; ISO 62
1.5 %

@Temperature 23.0 °C
1.5 %

@Temperature 73.4 °F
Immersion 24h; ISO 62
2.2 %

@Temperature 23.0 °C
2.2 %

@Temperature 73.4 °F
Saturation, immersed; ISO 62
Mechanical Properties Metric English Comments
Hardness, Shore D 54

@Time 15.0 sec
54

@Time 0.00417 hour
ISO 868
Tensile Strength at Break 30.0 MPa

@Temperature 23.0 °C
4350 psi

@Temperature 73.4 °F
ISO 527 (1BA bar)
Tensile Stress 7.50 MPa

@Strain 5.00 %,
Temperature 23.0 °C
1090 psi

@Strain 5.00 %,
Temperature 73.4 °F
ISO 527 (1BA bar)
11.0 MPa

@Strain 10.0 %,
Temperature 23.0 °C
1600 psi

@Strain 10.0 %,
Temperature 73.4 °F
ISO 527 (1BA bar)
16.0 MPa

@Strain 50.0 %,
Temperature 23.0 °C
2320 psi

@Strain 50.0 %,
Temperature 73.4 °F
ISO 527 (1BA bar)
Elongation at Break >= 300 %

@Temperature 23.0 °C
>= 300 %

@Temperature 73.4 °F
nominal; ISO 527 (1BA bar)
>= 300 %

@Temperature 23.0 °C
>= 300 %

@Temperature 73.4 °F
ISO 527 (1BA bar)
Tensile Modulus 0.210 GPa

@Temperature 23.0 °C
30.5 ksi

@Temperature 73.4 °F
ISO 527
Charpy Impact, Notched 1.70 J/cm²

@Temperature -30.0 °C
8.09 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 215 °C
419 °F
10°C/min; ISO 11357-1/-3
Processing Properties Metric English Comments
Melt Temperature 230 °C
446 °F
Optimum; Extrusion
225 - 245 °C
437 - 473 °F
Extrusion
Drying Temperature 100 °C
212 °F
Extrusion
Dry Time 2.00 - 3.00 hour
2.00 - 3.00 hour
Extrusion
Moisture Content <= 0.080 %
<= 0.080 %
Extrusion
Descriptive Properties Value Comments
Generic TPC-ET
Part Marking Code >TPC-ET<
ISO 11469
Product Category Extrusion Resins
Resin Identification TPC-ET
ISO 1043