Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Austin Novel Materials Texalan® 690A Polyester and Polyether based TPU

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade , Thermoplastic Polyurethane (TPUR), Polyether Grade
Manufacturer Austin Novel Materials
Trade Name Texalan®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Austin Novel Materials Texalan® 690A Polyester and Polyether based TPU.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: A kind of custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech
Physical Properties Metric English Comments
Density 1.19 - 1.23 g/cc
0.0430 - 0.0444 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 87 - 93
87 - 93
ISO 7619
Tensile Strength >= 42.0 MPa
>= 6090 psi
ISO 37
Tensile Stress >= 8.00 MPa

@Strain 100 %
>= 1160 psi

@Strain 100 %
ISO 37
>= 16.0 MPa

@Strain 300 %
>= 2320 psi

@Strain 300 %
ISO 37
Elongation at Yield >= 550 %
>= 550 %
ISO 37
Tear Strength >= 70.0 kN/m
>= 399 pli
ISO 34
K Factor (Wear Factor) <= 55
<= 55
[mm<sup>3</sup>]; ISO 4649
Compression Set <= 40 %

@Temperature 70.0 °C
<= 40 %

@Temperature 158 °F
ISO 815
Users viewing this material also viewed the following: