Mechanical Properties Metric English Comments
Izod Impact, Notched 0.450 J/cm

@Temperature -20.0 °C
0.843 ft-lb/in

@Temperature -4.00 °F
ASTM D256
LATI LASTIROL R-V0 Polystyrene (PS) (UL94 V-0)  (discontinued **)
Lastirol thermoplastics are polystyrene (PS) products. The Lastirols feature excellent dimensional stability, good flowability, and can be molded without any particular problem. Glass fiber reinforc..
Izod Impact, Notched 0.450 J/cm

@Temperature -20.0 °C
0.843 ft-lb/in

@Temperature -4.00 °F
ASTM D256
LATI LASTIROL R-V2 Polystyrene (PS) (UL94 V-2)  (discontinued **)
Description: Lastirol thermoplastics are polystyrene (PS) products. The Lastirols feature excellent dimensional stability, good flowability, and can be molded without any particular problem. Glass f..
Izod Impact, Notched 0.450 J/cm

@Temperature 23.0 °C
0.843 ft-lb/in

@Temperature 73.4 °F
ASTM D256
LATI LATILUB 82-01M Nylon 12 Base, 1% Molybdenum Disulfide Self Lubricating Plastic  (discontinued **)
Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri..
Izod Impact, Notched 0.450 J/cm

@Temperature -30.0 °C
0.843 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Noryl V01505 PPE+HIPS
Noryl* V01505 is a 15% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t..
Izod Impact, Notched 0.450 J/cm

@Temperature -30.0 °C
0.843 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Noryl V01505 PPE+HIPS (Asia Pacific)
Noryl* V01505 is a 15% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t..
Izod Impact, Notched 0.450 J/cm

@Temperature -30.0 °C
0.843 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Ultem HFATX200 PEI+PCE
High flow Polyetherimide blend with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched 0.450 J/cm

@Temperature -30.0 °C
0.843 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Ultem HFATX200 PEI+PCE (Asia Pacific)
High flow Polyetherimide blend with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region.
Izod Impact, Notched 0.450 J/cm

@Temperature -30.0 °C
0.843 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Ultem HFATX200 PEI+PCE (Europe-Africa-Middle East)
High flow Polyetherimide blend with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Izod Impact, Notched 0.450 J/cm

@Temperature -30.0 °C
0.843 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS
Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a..
Izod Impact, Notched 0.450 J/cm

@Temperature -30.0 °C
0.843 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS (Europe-Africa-Middle East)
Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a..
Izod Impact, Notched 0.450 J/cm

@Temperature -40.0 °C
0.843 ft-lb/in

@Temperature -40.0 °F
Absolute Drying; ASTM-D256
Toyobo GLAMIDE® T-400G15 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Izod Impact, Notched 0.450 J/cm

@Temperature 23.0 °C
0.843 ft-lb/in

@Temperature 73.4 °F
Absolute Drying; ASTM-D256
Toyobo GLAMIDE® T-662 Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Izod Impact, Notched 0.450 J/cm

@Temperature -40.0 °C
0.843 ft-lb/in

@Temperature -40.0 °F
Practical Use (Water Absorption 2.0%); ASTM-D256
Toyobo GLAMIDE® T-777-02 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Izod Impact, Notched 0.450 J/cm

@Temperature -40.0 °C
0.843 ft-lb/in

@Temperature -40.0 °F
Practical Use (Water Absorption 3.5%); ASTM-D256
Toyobo GLAMIDE® T-803 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Izod Impact, Notched 0.450 J/cm

@Temperature -40.0 °C
0.843 ft-lb/in

@Temperature -40.0 °F
Practical Use (Water Absorption 3.0%); ASTM-D256
Toyobo GLAMIDE® T-808-02 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Izod Impact, Notched 0.450 J/cm

@Temperature -40.0 °C
0.843 ft-lb/in

@Temperature -40.0 °F
Practical Use; ASTM-D256
Toyobo GLAMIDE® TY-835TC Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Izod Impact, Notched 0.450 J/cm

@Temperature -20.0 °C
0.843 ft-lb/in

@Temperature -4.00 °F
ASTM D256
Total PPC 4720XWZ Polypropylene, Impact Copolymer
TOTAL Petrochemicals Polypropylene 4720XWZ is a nucleated impact copolymer with a Melt Flow index of 25 g/10 min.TOTAL Polypropylene 4720XWZ is characterized by improved stiffness, creep resistance,..
Izod Impact, Notched 0.450 J/cm

@Temperature -40.0 °C
0.843 ft-lb/in

@Temperature -40.0 °F
Practical Use (Water Absorption 1.8%); ASTM-D256
Toyobo GLAMIDE® T-422VOR Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Izod Impact, Notched 0.450 J/cm

@Temperature 23.0 °C
0.843 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Toyobo T-661 Nylon 66, Standard Grade (DAM)
Features: Non-reinforced, Standard GradeInformation provided by Toyobo.
Izod Impact, Notched 0.450 J/cm

@Temperature -20.0 °C
0.843 ft-lb/in

@Temperature -4.00 °F
ASTM D 638
Cossa Polimeri ESTAPROP 1000 V2 K Flame Retardant Polypropylene
PP copolymerFlame retardant class V2, PBDE free, good processability, good impact strengthInformation provided by Cossa Polimeri S.r.l.
Izod Impact, Notched 0.450 J/cm

@Temperature 23.0 °C
0.843 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Cossa Polimeri ESTAPROP 1040 V2 K Flame Retardant Polypropylene
PP copolymerFlame retardant class V2, halogen free, good mechanical characteristicsInformation provided by Cossa Polimeri S.r.l.
Izod Impact, Notched 0.450 J/cm

@Temperature 23.0 °C
0.843 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Cossa Polimeri ESTAPROP 1050 V0 HF K Flame Retardant Polypropylene
PP copolymerFlame retardant class V0, halogen free, excellent mechanical characteristics, excellent processabilityInformation provided by Cossa Polimeri S.r.l.
Izod Impact, Notched 0.450 J/cm

@Temperature 23.0 °C
0.843 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Braskem Symbios 3102 Polypropylene Terpolymer
Braskem Symbios 3102 is a medium melt flow rate terpolymer with a heat seal temperature below 110ºC on its non-treated face. It is designed for use as a heat sealing layer for cast film coextrusion..
Izod Impact, Notched 0.450 J/cm

@Temperature -20.0 °C
0.843 ft-lb/in

@Temperature -4.00 °F
ASTM D256
Carmel Olefins CAPILENE® SW 75 AV Polypropylene Impact Copolymer
Description: CAPILENE® SW 75 AV is a high melt flow rate, controlled rheology impact copolymer for injection molding. CAPILENE® SW 75 AV is nucleated with antistatic additivation. It is characte..
Izod Impact, Notched 0.450 J/cm

@Temperature -40.0 °C
0.843 ft-lb/in

@Temperature -40.0 °F
Absolute Drying; ASTM-D256
Toyobo GLAMIDE® T-401 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Izod Impact, Notched 0.450 J/cm

@Temperature -20.0 °C
0.843 ft-lb/in

@Temperature -4.00 °F
ASTM D256
LATI LASTIROL TR G/10-V1 10% Glass Fiber Reinforced Polystyrene (PS) (UL94 V-1)  (discontinued **)
Description: Lastirol thermoplastics are polystyrene (PS) products. The Lastirols feature excellent dimensional stability, good flowability, and can be molded without any particular problem. Glass f..
Izod Impact, Notched 0.450 J/cm

@Temperature -40.0 °C
0.843 ft-lb/in

@Temperature -40.0 °F
ASTM D256
LATI LARTON GCE/60 60% Mixed Glass Fiber and Special Mineral Filled Polyphenylene sulfide (PPS)  (discontinued
Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex..
Izod Impact, Notched 0.450 J/cm

@Temperature -30.0 °C
0.843 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS (Asia Pacific)
Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a..
Izod Impact, Notched 0.450 J/cm

@Temperature 23.0 °C
0.843 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Xenoy® X6320 PBT+PC
X6320 is a mineral filled PBT/PC resin developed for automotive painted doorhandles. Key advantages are excellent surface finish, easy processing and paint quality.This data was supplied by SABIC-IP..
Izod Impact, Notched 0.450 J/cm

@Temperature -30.0 °C
0.843 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Xenoy® X6320 PBT+PC
X6320 is a mineral filled PBT/PC resin developed for automotive painted doorhandles. Key advantages are excellent surface finish, easy processing and paint quality.This data was supplied by SABIC-IP..
Copyright © lookpolymers.com All Rights Reserved