Material Notes:
Braskem Symbios 3102 is a medium melt flow rate terpolymer with a heat seal temperature below 110ºC on its non-treated face. It is designed for use as a heat sealing layer for cast film coextrusion. This product does not have slip and anti-blocking agents so it's indicated for customized formularization. This product is appropriate for metallizing and lamination processes.
Physical Properties Metric English Comments
Density 0.902 g/cc
0.0326 lb/in³
ASTM-D792
Melt Flow 9.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
9.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM-D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 87
87
ASTM-D785
Tensile Strength, Yield 26.0 MPa
3770 psi
ASTM-D638
Elongation at Yield 13 %
13 %
ASTM-D638
Flexural Modulus 0.800 GPa
116 ksi
ASTM-D790
Izod Impact, Notched 0.180 J/cm

@Temperature -20.0 °C
0.337 ft-lb/in

@Temperature -4.00 °F
ASTM-D256
0.450 J/cm

@Temperature 23.0 °C
0.843 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 51.0 °C
124 °F
ASTM-D648
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
176 °F
ASTM-D648
Vicat Softening Point 123 °C

@Load 1.02 kg
253 °F

@Load 2.25 lb
ASTM-D1525