Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Murtfeldt Murflor® + Bronze Polytetrafluoroethylene, 60% Bronze

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , Polytetrafluoroethylene (PTFE), Bronze Filled
Manufacturer Murtfeldt Kunststoffe GmbH & Co
Trade Name Murflor®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Murtfeldt Murflor® + Bronze Polytetrafluoroethylene, 60% Bronze.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The addition of 60% bronze to the base material reduces the expansion coefficient and gives lower sliding wear.Special Properties:• Lower sliding wear than Murflor®• Good slide properties• Low stick/slip effect• Higher compressive strength than Murflor®Information provided by Murtfeldt Kunststoffe GmbH & Co. KG.
Physical Properties Metric English Comments
Density 3.88 g/cc
0.140 lb/in³
ISO 1183-1
Mechanical Properties Metric English Comments
Hardness, Shore D 68
68
DIN 53505
Tensile Strength, Yield 14.0 MPa
2030 psi
ISO 527-1/-2
Elongation at Break 140 %
140 %
ISO 527-1/-2
Modulus of Elasticity 1.38 GPa
200 ksi
Compressive Yield Strength 10.5 MPa

@Strain 1.00 %
1520 psi

@Strain 1.00 %
dry; ISO 604
Charpy Impact, Notched 1.10 J/cm²
5.23 ft-lb/in²
ISO 179-1/1eA
Coefficient of Friction, Dynamic 0.14
0.14
Sand Slurry 0.50
0.50
µm/km
Thermal Properties Metric English Comments
CTE, linear 95.0 µm/m-°C

@Temperature 23.0 - 100 °C
52.8 µin/in-°F

@Temperature 73.4 - 212 °F
Melting Point 330 °C
626 °F
ISO 11357-1
Maximum Service Temperature, Air 260 °C

@Time 7.20e+7 sec
500 °F

@Time 20000 hour
300 °C

@Time <=86400 sec
572 °F

@Time <=24.0 hour
Minimum Service Temperature, Air -200 °C
-328 °F
Glass Transition Temp, Tg 127 °C
261 °F
ISO 11357-1
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Surface Resistance >= 1.00e+13 ohm
>= 1.00e+13 ohm
Compliance Properties Metric English Comments
FDA No
No
Descriptive Properties Value Comments
Color Bronze
Users viewing this material also viewed the following: