Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plaskolite West Optix® CA-1000 IG Clear High Impact Acrylic Resin

Category Polymer , Thermoplastic , Acrylic (PMMA) , Acrylic, Gamma Radiation Resistant, Molded , Acrylic, Impact Modified, Molded
Manufacturer Plaskolite West, Inc.
Trade Name Optix®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plaskolite West Optix® CA-1000 IG Clear High Impact Acrylic Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High impact acrylic resin, injection molding and extrusion gradeApplications: A premium impact acrylic resin particularly suited for medical and food uses. This resin is suited for Gamma irradiation treatment. Meets FDA CFR-21 Sec 177.1010 for food use. Meets USP Plastic Class VI for medical use.
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
ASTM D792
Melt Flow 1.6 g/10 min
1.6 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 40.0 MPa
5800 psi
ASTM D638
Elongation at Break 40 %
40 %
ASTM D638
Modulus of Elasticity 1.38 GPa
200 ksi
ASTM D638
Flexural Strength 46.9 MPa
6800 psi
ASTM D790
Izod Impact, Notched 0.640 J/cm
1.20 ft-lb/in
ASTM D256
Gardner Impact 7.34 J
5.42 ft-lb
Falling Weight; ASTM D3029GB
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 78.0 °C
172 °F
ASTM D648
Vicat Softening Point 100 °C
212 °F
Rate A, ASTM D1525
Flammability, UL94 HB
HB
Optical Properties Metric English Comments
Transmission, Visible 90.8 %
90.8 %
ASTM D1003