Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 1.38 - 2.96 GPa | 200 - 430 ksi | Average value: 2.06 GPa Grade Count:13 |
Overview of materials for Acrylic, Gamma Radiation Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Gamma Radiation Resistant, Molded". Each property range of values reported is minimum and maxim.. |