Network Polymers NPP Nylon 66G13L

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 10% Glass Fiber Filled
Manufacturer Network Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Network Polymers NPP Nylon 66G13L.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: NylonInformation provided by Network Polymers Inc.
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
ASTM D792
Water Absorption 1.0 %
1.0 %
24 hours Immersion; ASTM D570
Linear Mold Shrinkage, Flow 0.0050 cm/cm
0.0050 in/in
1/8 in bar; ASTM D955
Linear Mold Shrinkage, Transverse 0.0090 cm/cm
0.0090 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 122
122
ASTM D785
Tensile Strength at Break 103 MPa
15000 psi
ASTM D638
Elongation at Break 2.0 - 4.0 %
2.0 - 4.0 %
ASTM D638
Flexural Strength 148 MPa
21500 psi
ASTM D790
Flexural Modulus 4.83 GPa
700 ksi
ASTM D790
Izod Impact, Notched 0.374 J/cm
0.700 ft-lb/in
1/8 in specimen; ASTM D256
Tensile Impact Strength 126 kJ/m²
60.0 ft-lb/in²
ASTM D1822
Thermal Properties Metric English Comments
Melting Point 255 °C
491 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 240 °C
464 °F
0.125 in bar; ASTM D648