Material Notes:
Description: Black NylonInformation provided by Network Polymers Inc.
Physical Properties Metric English Comments
Specific Gravity 1.38 g/cc
1.38 g/cc
ASTM D792
Water Absorption 0.70 %
0.70 %
24 hours Immersion; ASTM D570
Linear Mold Shrinkage, Flow 0.0020 cm/cm
0.0020 in/in
1/8 in bar; ASTM D955
Linear Mold Shrinkage, Transverse 0.0050 cm/cm
0.0050 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 99
99
ASTM D785
Tensile Strength at Break 200 MPa
29000 psi
ASTM D638
Elongation at Break 2.0 - 4.0 %
2.0 - 4.0 %
ASTM D638
Flexural Strength 283 MPa
41000 psi
ASTM D790
Flexural Modulus 9.31 GPa
1350 ksi
ASTM D790
Izod Impact, Notched 1.17 J/cm
2.20 ft-lb/in
1/8 in specimen; ASTM D256
Tensile Impact Strength 126 kJ/m²
60.0 ft-lb/in²
ASTM D1822
Thermal Properties Metric English Comments
Melting Point 255 °C
491 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 250 °C
482 °F
0.125 in bar; ASTM D648