Axiall 9275J Clear 38 Rigid PVC, Molding, Clear 38

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 9275J Clear 38 Rigid PVC, Molding, Clear 38.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Georgia Gulf 9275J Clear 38 is a food grade used for injection blow molded packages in critical medical, cosmetic and toiletry applications. All ingredients are FDA approved.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.33 g/cc
1.33 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 49.0 MPa
7100 psi
ASTM D-638
Tensile Modulus 2.83 GPa
410 ksi
ASTM D-638
Flexural Strength 89.6 MPa
13000 psi
ASTM D-790
Izod Impact, Notched 0.160 J/cm

@Thickness 6.35 mm
0.300 ft-lb/in

@Thickness 0.250 in
ASTM D-256
0.267 J/cm

@Thickness 3.17 mm
0.500 ft-lb/in

@Thickness 0.125 in
ASTM D-256
Tensile Impact Strength 126 kJ/m²
60.0 ft-lb/in²
ASTM D-1822
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 56.00 °C
132.8 °F
ASTM D-648
Optical Properties Metric English Comments
Haze 5.0 %

@Thickness 3.17 mm
5.0 %

@Thickness 0.125 in
pressed plaque; ASTM D-1003-61
Transmission, Visible 80 %

@Thickness 3.17 mm
80 %

@Thickness 0.125 in
pressed plaque; ASTM D-1003-61
Descriptive Properties Value Comments
Equilibrium Torque, meter-grams 900
Brabender Plastograph, No. 6 Roller Head, 190°C Bath, 57-g. Charge; 60/43 rpm
Melt Flow, seconds 83
ASTM D-1238
Stability Time, minutes 62