Georgia Gulf 7140 is a special purpose rigid PVC compound designed for applications requiring the following properties: WeatherabilityGlossImpact Strength & ToughnessFlame RetardantChemical ResistanceThermoformabilityExtrudability in ProfileMoldability in FittingsInformation provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.47 g/cc
1.47 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 112
112
ASTM D-785
Hardness, Shore D 83
83
ASTM D-2240
Tensile Strength, Yield 44.8 MPa
6500 psi
ASTM D-638
Tensile Modulus 2.62 GPa
380 ksi
ASTM D-638
Flexural Strength 83.4 MPa
12100 psi
ASTM D-790
Flexural Modulus 2.76 GPa
400 ksi
ASTM D-790
Izod Impact, Notched 8.01 J/cm
15.0 ft-lb/in
ASTM D-256
Tensile Impact Strength 126 kJ/m²
60.0 ft-lb/in²
ASTM D-1822
Thermal Properties Metric English Comments
CTE, linear 72.0 µm/m-°C

@Temperature 20.0 °C
40.0 µin/in-°F

@Temperature 68.0 °F
ASTM D-696
Deflection Temperature at 1.8 MPa (264 psi) 72.2 °C
162 °F
ASTM D-648
Flammability, UL94 V-0
V-0
At 0.030 inch
Descriptive Properties Value Comments
Cell Classification 14344
ASTM D-1784