Material Notes:
Product Description: AP60-007 is a medium molecular weight distribution high density polyethylene homopolymer. It possesses excellent processing uniformity and produces bottles with excellent appearance and rigidity. AP60-007 offers the maximum in barrier properties available in high density polyethylene, and imparts minimum odor and taste to the packaged product.Availability: Latin America, North America and South America Additive: Thermal Stabilizer: YesAntistatic: NoApplications: Food packagingLiquid Food Containers for Milk, Water and JuicesThermoformed PartsInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.963 g/cc
0.0348 lb/in³
ASTM D4883
ESCR 100% Igepal® 10 hour
10 hour
ASTM D1963
Melt Flow 0.73 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.73 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 31.7 MPa
4600 psi
ASTM D638
Elongation at Break 350 %
350 %
ASTM D638
Flexural Modulus 1.72 GPa
250 ksi
ASTM D790
Tensile Impact Strength 126 kJ/m²
60.0 ft-lb/in²
ASTM D1822
Thermal Properties Metric English Comments
Vicat Softening Point 127 °C
261 °F
ASTM D1525
Brittleness Temperature <= -76.1 °C
<= -105 °F
ASTM D746