Polymer Property : Compressive Strength = 2000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 13.8 MPa
2000 psi
Break; Mixed 1:2; TM R050-38
Resinlab® EP1215 Clear Unfilled Epoxy Structural Adhesive
Resinlab™ EP1215 Clear is a two part unfilled epoxy structural adhesive designed for bonding applications requiring high strength and good impact resistance. It cures completely at room temperature..
Compressive Strength 13.8 MPa
2000 psi
Ultimate; Mixed 1:2; TM R050-38
Resinlab® EP1215 Clear Unfilled Epoxy Structural Adhesive
Resinlab™ EP1215 Clear is a two part unfilled epoxy structural adhesive designed for bonding applications requiring high strength and good impact resistance. It cures completely at room temperature..
Compressive Strength 13.8 MPa
2000 psi
Maximum working pressure
Potters Industries Q-Cel® 6042S
Performance Benefits: A low-density, performance-enhancing additive.Fewer defects: excellent mold flow, uniform dispersionReduced compound density and viscosityIncreased acoustic and thermal insulat..
Compressive Strength <= 13.8 MPa
<= 2000 psi
Working pressure
Potters Industries Q-Cel® 7040S Hollow Engineered Glass Microspheres
Q-CEL® hollow glass microspheres are alternatives to conventional fillers and additives such as silicas, calcium carbonates, talc, clay, etc. A variety of particle sizes, densities and strengths me..
Compressive Strength 13.8 MPa
2000 psi
Break; TM R050-38
Resinlab® EP1295 Black Medium Viscosity, Halogen Free, Flame Retardant Epoxy Casting Resin
Resinlab™ EP1295 Black is a medium viscosity, halogen free, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (..
Compressive Strength 13.8 MPa
2000 psi
SPHERE ONE EXTENDOSPHERESâ„¢ 300/600 Hollow Spheres
EXTENDOSPHERESâ„¢300/600 are efficient, lightweight additives for most resin systems. When Extendospheresâ„¢ replace heavier, more expensive components on an equivalent volume basis, they can ..
Compressive Strength 13.8 - 27.6 MPa
2000 - 4000 psi
Crush Strength
Trelleborg Fillite® 160W Alumino-silicate Cenospheres
Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio..
Compressive Strength 13.8 - 27.6 MPa
2000 - 4000 psi
Crush Strength
Trelleborg Fillite® SGHA (500HA) Alumino-silicate Cenospheres
Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio..
Compressive Strength 13.8 - 27.6 MPa
2000 - 4000 psi
Crush Strength
Trelleborg Fillite® 300W Alumino-silicate Cenospheres
Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio..
Compressive Strength 13.8 - 103 MPa
2000 - 15000 psi
Du-Co Ceramics S-461 Magnesia
Du-Co Ceramics Company manufactures a variety of crushable ceramic materials for use worldwide in cartridge heaters, thermocouples, and mineral insulated cable. The crushable ceramic products are cu..
Compressive Strength 13.8 - 41.4 MPa
2000 - 6000 psi
Du-Co Ceramics S-570 Silica
Du-Co Ceramics Company manufactures a variety of crushable ceramic materials for use worldwide in cartridge heaters, thermocouples, and mineral insulated cable. The crushable ceramic products are cu..
Compressive Strength 13.8 MPa
2000 psi
3M HGS2000 Glass Bubbles
3M™ Glass Bubbles HGS Series are engineered hollow glass spheres for use as a density reducing agent for oil and gas drilling fluids and drilling cements. The spherical shape of 3M glass bubbles of..
Compressive Strength 13.8 MPa
2000 psi
3M S32 Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
Compressive Strength 13.8 MPa
2000 psi
Aremco Ceramacast™ 675 High Temperature Potting & Casting Material Aluminum Nitride
Fine grain aluminum nitride castable with high thermal conductivity
Compressive Strength 13.8 MPa
2000 psi
Aremco Ceramacast™ 675-N High Temperature Potting & Casting Material Aluminum Nitride
Fine grain aluminum nitride castable with high thermal conductivity.
Compressive Strength 13.8 - 20.7 MPa
2000 - 3000 psi
Abatron AboCast 7802-1/AboCure 50-3 (80 pbw) Epoxy
AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 50-3 is a clear, slow converter for lower rigidity. It has an HDT of 60°C, variable ratio, ..
Compressive Strength 13.8 - 20.7 MPa
2000 - 3000 psi
Abatron AboCast 7802-1/AboCure 7804-4 (80 pbw) Epoxy
AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 7804-4 a clear, more accelerated converter for lower rigidity. It has an HDT of 60°C, varia..
Compressive Strength 13.8 - 20.7 MPa
2000 - 3000 psi
ASTM D695
Arkema Group Kynar Super Flex® 2500 PVDF Copolymer  (discontinued **)
Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry..
Compressive Strength >= 13.8 MPa
>= 2000 psi
ASTM C365
Touchstone CFOAM® 25 Structural Carbon Foam
CFOAM, developed by Touchstone Research Laboratory, Ltd., is a next generation structural material which is inexpensive, lightweight, fire-resistant, impact-absorbing, and which can be thermally ins..
Compressive Strength 13.8 MPa
2000 psi
Resinlab® UR1049 MDI Based Rigid Polyurethane Foam System
Resinlab™ UR 1049 is a, two component, water blown, 4 lb per cubic foot, MDI based rigid polyurethane foam system. It is designed to cure completely at room temperature. Being of a closed cell stru..