Polymer Property : Compressive Strength = 6000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 31.0 - 41.4 MPa
4500 - 6000 psi
ASTM D695
Arkema Group Kynar Flex® 2900 PVDF Copolymer  (discontinued **)
Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry..
Compressive Strength 31.0 - 41.4 MPa
4500 - 6000 psi
ASTM D695
Arkema Group Kynar Flex® 3120 PVDF Copolymer  (discontinued **)
Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry..
Compressive Strength 13.8 - 41.4 MPa
2000 - 6000 psi
Du-Co Ceramics S-570 Silica
Du-Co Ceramics Company manufactures a variety of crushable ceramic materials for use worldwide in cartridge heaters, thermocouples, and mineral insulated cable. The crushable ceramic products are cu..
Compressive Strength 27.6 - 41.4 MPa
4000 - 6000 psi
ASTM C133
Ceradyne Thermo-Sil® Castable 120 Fused Silica
Fused Silica is an excellent thermal insulator with an extremely low coefficient of thermal expansion. It is excellent for thermal shock applications. The key characteristics of this material are:Hi..
Compressive Strength 27.6 - 41.4 MPa
4000 - 6000 psi
ASTM C133
Ceradyne Thermo-Sil® Castable TG Fused Silica
Fused Silica is an excellent thermal insulator with an extremely low coefficient of thermal expansion. It is excellent for thermal shock applications. The key characteristics of this material are:Hi..