Touchstone CFOAM® 25 Structural Carbon Foam

Category Carbon , Other Engineering Material , Composite Core Material
Manufacturer Touchstone Research Laboratory
Trade Name CFOAM®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Touchstone CFOAM® 25 Structural Carbon Foam.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CFOAM, developed by Touchstone Research Laboratory, Ltd., is a next generation structural material which is inexpensive, lightweight, fire-resistant, impact-absorbing, and which can be thermally insulating or conducting and whose electrical conductivity can be varied over seven orders of magnitude. It can be fabricated in a variety of shapes, sizes, and densities to meet the property requirements of specific applications.These foams will not off-gas at elevated temperatures and will not support ignition. Unlike most metals and ceramics, CFOAM mechanical properties do not deteriorate with increased temperature if protected from oxidization, making carbon foams an attractive thermal protection material. Carbon foams also are tolerant to impact damage and can be repaired in-place using carbonaceous adhesives. They can be bonded easily to dissimilar materials, such as metals or PMCs, for oxidation or further impact protection, respectively.Results from ASTM E1354, ASTM E1515, MIL-STD-1623, Coast Guard IMO, and FTP Code Part I and Part III indicate that CFOAM will pass all key fire tests including radiant panel, smoke generation, toxicity, cone calorimeter, fire resistance, and room corner tests.Information provided by Touchstone Research Laboratory.
Physical Properties Metric English Comments
Density 0.400 g/cc
0.0145 lb/in³
ASTM D1622
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate >= 3.45 MPa
>= 500 psi
ASTM C297
Tensile Modulus 0.827 GPa
120 ksi
ASTM C297
Compressive Strength >= 13.8 MPa
>= 2000 psi
ASTM C365
Compressive Modulus 0.827 GPa
120 ksi
ASTM C365
Shear Strength >= 2.07 MPa
>= 300 psi
Torsional Shear
Thermal Properties Metric English Comments
CTE, linear 5.76 µm/m-°C

@Temperature 20.0 °C
3.20 µin/in-°F

@Temperature 68.0 °F
ASTM E228
Thermal Conductivity 0.250 - 25.0 W/m-K
1.74 - 174 BTU-in/hr-ft²-°F
Tailorable; ASTM E1225
Maximum Service Temperature, Air 600.0 °C
1112 °F
Maximum Service Temperature, Inert 3000 °C
5430 °F
Electrical Properties Metric English Comments
Electrical Resistivity 0.0100 - 1.00e+7 ohm-cm
0.0100 - 1.00e+7 ohm-cm
Tailorable; ASTM D4496