Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SPHERE ONE EXTENDOSPHERESâ„¢ 300/600 Hollow Spheres

Category Ceramic , Oxide , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Sphere One Inc
Trade Name EXTENDOSPHERES™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SPHERE ONE EXTENDOSPHERESâ„¢ 300/600 Hollow Spheres.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
EXTENDOSPHERESâ„¢300/600 are efficient, lightweight additives for most resin systems. When Extendospheresâ„¢ replace heavier, more expensive components on an equivalent volume basis, they can reduce raw material costs as well as density. EXTENDOSPHERESâ„¢ 300/600 hollow spheres are gray, low-cost, low-density ceramic hollow spheres. With a density of 0.80 g/cm3, these hollow spheres are ideal for specialty applications where larger particle size is required.Information provided by Sphere One Inc.
Physical Properties Metric English Comments
Bulk Density 0.300 g/cc
0.0108 lb/in³
Density 0.800 g/cc
0.0289 lb/in³
Particle Size 400 µm
400 µm
Average Mean
300 - 600 µm
300 - 600 µm
Mechanical Properties Metric English Comments
Hardness, Mohs 5.0
5.0
Compressive Strength 13.8 MPa
2000 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1200 °C
2190 °F
Deformation temp
Descriptive Properties Value Comments
Color gray
Physical Form Free-Flowing Powder
Shell Thickness Approx. 10% of diameter
Users viewing this material also viewed the following: