Mechanical Properties Metric English Comments
Compressive Strength 13.8 - 27.6 MPa
2000 - 4000 psi
Crush Strength
Trelleborg Fillite® 160W Alumino-silicate Cenospheres
Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio..
Compressive Strength 13.8 - 27.6 MPa
2000 - 4000 psi
Crush Strength
Trelleborg Fillite® SGHA (500HA) Alumino-silicate Cenospheres
Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio..
Compressive Strength 13.8 - 27.6 MPa
2000 - 4000 psi
Crush Strength
Trelleborg Fillite® 300W Alumino-silicate Cenospheres
Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio..
Compressive Strength 20.7 - 27.6 MPa
3000 - 4000 psi
Abatron AboCast 7802-1/AboCure 7804-3 (80 pbw) Epoxy
AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 7804-3 a clear, slightly accelerated converter for lower rigidity. It has an HDT of 60°C, v..