Physical Properties Metric English Comments
Viscosity Test 95.0 - 160 cm³/g
95.0 - 160 cm³/g
Average value: 138 cm³/g Grade Count:9
Overview of materials for Nylon 6, Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum values..
Viscosity Test 115 - 160 cm³/g
115 - 160 cm³/g
Average value: 131 cm³/g Grade Count:6
Overview of materials for Nylon 6-3
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6-3". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..
Viscosity Test 140 - 160 cm³/g
140 - 160 cm³/g
Sulphuric Acid; EN ISO 307
Domo Domamid® 39 APBH Polyamide 6.6
DOMAMID® 39APBH are Polyamide 6.6 pellets produced from AH-salt.Applications: Injection moulding CompoundingExtrusionInformation provided by Domo
Viscosity Test 140 - 160 cm³/g
140 - 160 cm³/g
Sulphuric Acid; EN ISO 307
Domo Domamid® 50 ABH Polyamide 6.6
DOMAMID® 50ABH are Polyamide 6.6 pellets produced from AH-salt.Applications: Injection moulding CompoundingExtrusionInformation provided by Domo