DuPont Performance Polymers Zytel® 73G35HSL BK262 Nylon 6  (Unverified Data**)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 40% Glass Fiber Filled
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Zytel® 73G35HSL BK262 Nylon 6  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Zytel® 73G35HSL BK262 is a 35% glass fiber reinforced, heat stabilized, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
DAM; ISO 1183
Filler Content 35 %
35 %
DAM
Water Absorption 1.8 %

@Thickness 1.00 mm,
Temperature 23.0 °C
1.8 %

@Thickness 0.0394 in,
Temperature 73.4 °F
Equilibrium 50%RH; DAM; ISO 62, Similar to
5.8 %

@Thickness 1.00 mm,
Temperature 23.0 °C
5.8 %

@Thickness 0.0394 in,
Temperature 73.4 °F
Saturation, immersed; DAM; ISO 62, Similar to
Linear Mold Shrinkage, Flow 0.0020 cm/cm

@Thickness 2.00 mm
0.0020 in/in

@Thickness 0.0787 in
DAM; ISO 294-4
Linear Mold Shrinkage, Transverse 0.010 cm/cm

@Thickness 2.00 mm
0.010 in/in

@Thickness 0.0787 in
DAM; ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 115 MPa

@Temperature 23.0 °C
16700 psi

@Temperature 73.4 °F
50%RH; ISO 527
190 MPa

@Temperature 23.0 °C
27600 psi

@Temperature 73.4 °F
DAM; ISO 527
Elongation at Break 3.2 %

@Temperature 23.0 °C
3.2 %

@Temperature 73.4 °F
DAM; ISO 527
5.0 %

@Temperature 23.0 °C
5.0 %

@Temperature 73.4 °F
50%RH; ISO 527
Tensile Modulus 6.50 GPa

@Temperature 23.0 °C
943 ksi

@Temperature 73.4 °F
50%RH; ISO 527
11.0 GPa

@Temperature 23.0 °C
1600 ksi

@Temperature 73.4 °F
DAM; ISO 527
Izod Impact, Notched (ISO) 13.0 kJ/m²

@Temperature 23.0 °C
6.19 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 180/1A
20.0 kJ/m²

@Temperature 23.0 °C
9.52 ft-lb/in²

@Temperature 73.4 °F
50%RH; ISO 180/1A
Charpy Impact Unnotched 9.00 J/cm²

@Temperature 23.0 °C
42.8 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 179/1eU
9.00 J/cm²

@Temperature 23.0 °C
42.8 ft-lb/in²

@Temperature 73.4 °F
50%RH; ISO 179/1eU
9.00 J/cm²

@Temperature -30.0 °C
42.8 ft-lb/in²

@Temperature -22.0 °F
50%RH; ISO 179/1eU
9.00 J/cm²

@Temperature -30.0 °C
42.8 ft-lb/in²

@Temperature -22.0 °F
DAM; ISO 179/1eU
Charpy Impact, Notched 1.00 J/cm²

@Temperature -30.0 °C
4.76 ft-lb/in²

@Temperature -22.0 °F
50%RH; ISO 179/1eA
1.00 J/cm²

@Temperature -30.0 °C
4.76 ft-lb/in²

@Temperature -22.0 °F
DAM; ISO 179/1eA
1.10 J/cm²

@Temperature -40.0 °C
5.23 ft-lb/in²

@Temperature -40.0 °F
DAM; ISO 179/1eA
1.20 J/cm²

@Temperature -40.0 °C
5.71 ft-lb/in²

@Temperature -40.0 °F
50%RH; ISO 179/1eA
1.60 J/cm²

@Temperature 23.0 °C
7.61 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 179/1eA
2.20 J/cm²

@Temperature 23.0 °C
10.5 ft-lb/in²

@Temperature 73.4 °F
50%RH; ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 221 °C
430 °F
10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
428 °F
DAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 208 °C
406 °F
DAM; ISO 75-1/-2
UL RTI, Electrical 65.0 °C

@Thickness 1.50 mm
149 °F

@Thickness 0.0591 in
DAM; UL 746B
UL RTI, Mechanical with Impact 65.0 °C

@Thickness 1.50 mm
149 °F

@Thickness 0.0591 in
DAM; UL 746B
UL RTI, Mechanical without Impact 65.0 °C

@Thickness 1.50 mm
149 °F

@Thickness 0.0591 in
DAM; UL 746B
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
DAM; UL94
HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
DAM; IEC 60695-11-10
Processing Properties Metric English Comments
Melt Temperature 270 °C
518 °F
DAM; Optimum
260 - 280 °C
500 - 536 °F
DAM
Mold Temperature 70.0 - 120 °C
158 - 248 °F
DAM
100 °C
212 °F
DAM; optimum
Drying Temperature 80.0 °C
176 °F
DAM
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
DAM
Moisture Content <= 0.20 %
<= 0.20 %
DAM
Descriptive Properties Value Comments
Additive Heat Stabilizer
DAM
Lubricant
DAM
Appearance Black Color
DAM
Drying Recommended Yes, if moisture content of resin exceeds recommended level
DAM
Features Chemical Resistance, Good
DAM
Fatigue Resistant
DAM
Fuel Resistant
DAM
Grease Resistant
DAM
Heat Aging Resistance, Good
DAM
Heat Stabilized
DAM
Oil Resistant
DAM
Thermal Aging Resistance, Good
DAM
Filler Glass fiber reinforcement
DAM
Forms Pellets
DAM
Generic Nylon 6
DAM
Material Status Current
DAM
Part Marking Code >PA6-GF35<
ISO 11469; DAM
Polymer Family Polyamide
DAM
Polymer Type PA6
DAM
Processing Method Injection Molding
DAM
Product Category Glass Reinforced Resins
DAM
Region Available - Global Yes
DAM
Resin Identification PA6-GF35
ISO 1043; DAM
RoHS Compliance Contact Manufacturer
DAM
Uses Appliance Components
DAM
Automotive Applications
DAM
Electrical/Electronic Applications
DAM
High Gloss Applications
DAM
Industrial Applications
DAM