Polymer Property : Melt Flow = 7.0 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 5.0 - 7.0 g/10 min
5.0 - 7.0 g/10 min
(Condition L) ASTM D-1238
Multibase Multi-Flex® TPE A 8615 BLK
This material is currently used in caster wheels where higher abrasion resistance is required. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Melt Flow 4.5 - 7.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
4.5 - 7.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238/L
NIZHNEKAMSKNEFTEKHIM PP 1500L (C30G) Propylene Homopolymer
Product obtained by polymerization of propylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation resistance when P..
Melt Flow 5.0 - 7.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
5.0 - 7.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238/L
NIZHNEKAMSKNEFTEKHIM PP 4210L (EP2C30F) Propylene and Ethylene Copolymer
Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation r..
Melt Flow 5.0 - 7.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
5.0 - 7.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238/L
NIZHNEKAMSKNEFTEKHIM PP 7445L (EPC57MA) Propylene and Ethylene Block Polymer
Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation r..
Melt Flow 3.0 - 7.0 g/10 min
3.0 - 7.0 g/10 min
ASTM D1238
Polymer Resources PCSF-FR G30 Polycarbonate, 30% Glass Reinforced Structural Foam Grade
Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Foam grades tested with foamed parts with a 10% weight reduction rel..
Melt Flow 2.0 - 7.0 g/10 min

@Load 11.6 kg,
Temperature 250 °C
2.0 - 7.0 g/10 min

@Load 25.6 lb,
Temperature 482 °F
ASTM D1238
Polymer Resources PPX-GP5 Modified-PPO, General Purpose
Modified-Polyphenylene Oxide, General Purpose, 270F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati..
Melt Flow 3.0 - 7.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
3.0 - 7.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Ravago Manufacturing Americas Hylex® P1010G30 HB Polycarbonate, 30% Fiberglass Reinforced
Information provided by Ravago.
Melt Flow 3.0 - 7.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
3.0 - 7.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Ravago Manufacturing Americas Hylex® P1310G30 HB Polycarbonate, 30% Fiberglass Reinforced, UV Stabilized
Information provided by Ravago.
Melt Flow 6.0 - 7.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
6.0 - 7.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
FKuR Kunststoff Terralene® HD 3505 Biobased Polyethylene
With the brand name Terralene® FKuR offers biobased polyethylene compounds made using Braskem's Green PE. When compared to conventional polyethylene (PE), the main difference is that the ethanol..
Melt Flow 4.1 - 7.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
4.1 - 7.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Iran Petrochemical (PCC) PC 0407 Polycarbonate
Suitable for extrusion, injection, and blow moldingInformation provided by Iran Petrochemical Commercial Co.
Melt Flow 4.0 - 7.0 g/10 min

@Load 2.16 kg,
Temperature 235 °C
4.0 - 7.0 g/10 min

@Load 4.76 lb,
Temperature 455 °F
ASTM D1238
Gromax CCP PBT 1100-211X
Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce..
Melt Flow 2.0 - 7.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
2.0 - 7.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
LTL Color Compounds Surlyn Reflection Series® SURSG201UG Surlyn Resin/Nylon 6 Alloy
A patented alloy of DuPont™ Surlyn® resin and nylon 6 for applications that require a high gloss, molded in color surface finish directly from the mold.All information provided by LTL Color ..
Melt Flow 3.0 - 7.0 g/10 min

@Load 2.16 kg,
Temperature 150 °C
3.0 - 7.0 g/10 min

@Load 4.76 lb,
Temperature 302 °F
Taiwan Sheen Soon Sheenthane® AH-782 TPU for Hotmelt Adhesive
Thermoplastic polyurethane elastomer for hotmelt adhesiveNon-yellowing, aliphatic gradeExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized...
Melt Flow 3.0 - 7.0 g/10 min
3.0 - 7.0 g/10 min
Cond L; ASTM D1238
Washington Penn PPH2TF-2B Polypropylene, 20% Talc Filled
Injection Molding Grade. Heat Stabilized. Meets Ford ESH-M4D293-B Spec.Applications: AC Blower wheels, parts and appliances.Data provided by Washington Penn Plastic Co., Inc.
Melt Flow 4.0 - 7.0 g/10 min
4.0 - 7.0 g/10 min
Cond L; ASTM D1238
Washington Penn PPH5CF75 Polypropylene, 75% Calcium Carbonate Filled Concentrate
UV Stabilized.Applications: ShelvingData provided by Washington Penn Plastic Co., Inc.
Melt Flow 5.0 - 7.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
5.0 - 7.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D 1238
RTP Company RTP 154 HI UV Polypropylene (PP), Copolymer - Flame Retardant - UV Stabilized
The RTP 154 family of compounds are flame retarded, unreinforced polypropylene materials. They offer improved physical properties, low specific gravity and excellent moldability vs. traditional V-0..
Melt Flow 5.0 - 7.0 g/10 min
5.0 - 7.0 g/10 min
ISO 1133
Chengdu Polyster H4040 Thermoplastic Polyether-ester Elastomer (TPEE)
Low modulus molding and injection grade. Contains improved color- stable antioxidants. Excellent flex resistance, especially at low temperatures. Moldable even in thin sections. Can be used in light..
Melt Flow 5.0 - 7.0 g/10 min
5.0 - 7.0 g/10 min
Biomer P240 PHB Biodegradable Polymer
PHB is a isotactic, absolutely linear, thermoplastic homopolyester built of 3-hydroxy butyric acid. The formula of the subunit is -[O-CH(CH3)-CH2-CO]-. PHB is free from even traces of catalysts. P..
Melt Flow 3.0 - 7.0 g/10 min
3.0 - 7.0 g/10 min
Asahi Glass Fluon® P-65P PFA Perfluoropolymer
Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character..
Melt Flow 3.0 - 7.0 g/10 min
3.0 - 7.0 g/10 min
Asahi Glass Fluon® P-805UP PFA Perfluoropolymer
Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character..
Melt Flow 3.0 - 7.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.0 - 7.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
AKG Polymers Vision PP PPH Jazz0502dark Polypropylene Homopolymer Compound
Vision consists of a complete assortment of high-quality compounds based on industrial PP waste.Applications: Automotive, Non-food packaging, Storage/transport systems, Road and hydraulic Engineerin..
Melt Flow 2.0 - 7.0 g/10 min

@Load 5.00 kg,
Temperature 232 °C
2.0 - 7.0 g/10 min

@Load 11.0 lb,
Temperature 450 °F
ASTM D1238
Arkema Group KYNAR® EXAD 3000 Polyvinylidene Fluoride - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Extrusion aid, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanic..
Melt Flow 3.0 - 7.0 g/10 min

@Load 2.16 kg,
Temperature 280 °C
3.0 - 7.0 g/10 min

@Load 4.76 lb,
Temperature 536 °F
ASTM D1238
E-Polymers EFLEX® M100 Ethylene Octene Copolymer
M-series: E-FLEX M series resins are a maleic anhydride grafted (MAH) polymer concentrate designed as synthetic rubber and polyolefin manufactured by E-Polymers. It offers excellent adhesion to nyl..
Melt Flow 3.0 - 7.0 g/10 min
3.0 - 7.0 g/10 min
ASTM D1238
S&E Specialty Polymers GPP1001V0M-HCO PP
Application: A polypropylene compound designed for injection molded industrial battery, electrical housing or appliance applications.  It affords medium impact resistance with a high level of flam..
Melt Flow 2.0 - 7.0 g/10 min
2.0 - 7.0 g/10 min
ASTM D1238
Polymer Resources PPX-GP5 Modified PPO, General Purpose with HDT of 270 F  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Melt Flow 6.0 - 7.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
6.0 - 7.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Granulate; ISO 1133/H
SYNTHOS Krasten® 552M High Impact Polystyrene
High impact grade with a wide range of Applications. Processed mainly by injection moulding. Production of consumer goods and technical parts subjected to increased mechanical stress. Good results i..