Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Multibase Multi-Flex® TPE A 8615 BLK

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Multibase
Trade Name Multi-Flex® TPE
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® TPE A 8615 BLK.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This material is currently used in caster wheels where higher abrasion resistance is required. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.02 g/cc
0.0368 lb/in³
ASTM D792
Melt Flow 5.0 - 7.0 g/10 min
5.0 - 7.0 g/10 min
(Condition L) ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore A 86
86
10 sec; ASTM D-2240
Tensile Strength, Ultimate 7.60 MPa
1100 psi
ASTM D412
Elongation at Break 780 %
780 %
ASTM D412
Flexural Strength 3.00 MPa
435 psi
ASTM D790
Flexural Modulus 0.0897 GPa
13.0 ksi
method 1, Proc.B; ASTM D-790
Tear Strength 48.2 kN/m
275 pli
ASTM D624
Copyright © lookpolymers.com All Rights Reserved