Material Notes:
Application: A polypropylene compound designed for injection molded industrial battery, electrical housing or appliance applications.  It affords medium impact resistance with a high level of flame retardancy. Available in a wide spectrum of colors.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 0.960 - 1.00 g/cc
0.960 - 1.00 g/cc
ASTM D792
Melt Flow 3.0 - 7.0 g/10 min
3.0 - 7.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 18.6 MPa
>= 2700 psi
ASTM D638
Elongation at Break >= 50 %
>= 50 %
ASTM D638
Flexural Modulus >= 1.21 GPa
>= 175 ksi
tangent; ASTM D790
Izod Impact, Notched >= 0.400 J/cm
>= 0.750 ft-lb/in
ASTM D256
Dart Drop, Total Energy >= 20.3 J
>= 15.0 ft-lb
ASTM D5420
Thermal Properties Metric English Comments
Flammability Test 5.0

@Thickness 1.59 mm
5.0

@Thickness 0.0625 in
Oxygen Index >= 28 %
>= 28 %
ASTM D2863
Users viewing this material also viewed the following: