Physical Properties Metric English Comments
Viscosity 450000 - 920000 cP

@Temperature 400 - 400 °C
450000 - 920000 cP

@Temperature 752 - 752 °F
Average value: 513000 cP Grade Count:2
Overview of materials for Polyetheretherketone, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu..
Viscosity 450000 - 920000 cP

@Shear Rate 1000 - 1000 1/s
450000 - 920000 cP

@Shear Rate 1000 - 1000 1/s
Average value: 513000 cP Grade Count:2
Overview of materials for Polyetheretherketone, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu..
Viscosity 450000 cP

@Shear Rate 1000 1/s,
Temperature 400 °C
450000 cP

@Shear Rate 1000 1/s,
Temperature 752 °F
Melt
Solvay Specialty Polymers AvaSpire® AV-722 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-722 is an unreinforced polyaryletherketone (PAEK) that offers improved economics relative to PEEK while retaining most of PEEK's key performance attributes. AV-722 resin has been formula..
Viscosity 450000 cP

@Shear Rate 1000 1/s,
Temperature 400 °C
450000 cP

@Shear Rate 1000 1/s,
Temperature 752 °F
Melt; ASTM D3835
Solvay Specialty Polymers AvaSpire® AV-750 GF40 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-750 GF40 is a 40% glass reinforced polyaryletherketone (PAEK) designed to fill the marketplace need for a lower-priced PEEK (polyetheretherketone). This resin provides the typical chemic..
Viscosity 450000 cP

@Shear Rate 1000 1/s,
Temperature 400 °C
450000 cP

@Shear Rate 1000 1/s,
Temperature 752 °F
Melt; ASTM D3835
Solvay Specialty Polymers KetaSpire® KT-880 CF30 Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-880 CF30 is a high flow, 30% carbon fiber reinforced grade of polyetheretherketone (PEEK). Carbon-fiber reinforcement of KetaSpire PEEK provides the maximum levels of mechanical propert..
Viscosity 450000 cP

@Temperature 400 °C
450000 cP

@Temperature 752 °F
Melt; ISO 11443
Victrex® PEEK 600P Polyetheretherketone  (discontinued **)
Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, coarse powder for extrusion compounding, low flow, FDA food contact complian..
Viscosity 450000 cP

@Temperature 400 °C
450000 cP

@Temperature 752 °F
Melt; ISO 11443
Victrex® PEEK 600PF Polyetheretherketone  (discontinued **)
Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, fine powder for compression compounding, low flow, FDA food contact complian..
Viscosity 450000 cP

@Temperature 400 °C
450000 cP

@Temperature 752 °F
melt; ISO 11443
Victrex® PEEK -HT™ 22GL30 Polyetherketone, 30% Glass Fiber Reinforced
Product Description:High performance thermoplastic material, 30% glass fibre reinforced PolyEtherKetone (PEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact comp..
Viscosity 450000 cP

@Shear Rate 1000 1/s,
Temperature 400 °C
450000 cP

@Shear Rate 1000 1/s,
Temperature 752 °F
Melt Viscosity; ASTM D3835
Solvay Specialty Polymers AvaSpire® AV-722 Polyaryletherketone (PAEK)
AvaSpire® AV-722 is an unreinforced polyaryletherketone (PAEK) that offers improved economics relative to PEEK while retaining most of PEEK's key performance attributes. AV-722 resin has been for..
Viscosity 450000 cP

@Shear Rate 1000 1/s,
Temperature 400 °C
450000 cP

@Shear Rate 1000 1/s,
Temperature 752 °F
Melt Viscosity; ASTM D3835
Solvay Specialty Polymers AvaSpire® AV-750 GF40 Polyaryletherketone (PAEK), 40% Glass Fiber
AvaSpire® AV-750 GF40 is a 40% glass reinforced polyaryletherketone (PAEK) designed to fill the marketplace need for a lower-priced PEEK (polyetheretherketone). This resin provides the typical ch..
Viscosity 450000 cP

@Shear Rate 1000 1/s,
Temperature 400 °C
450000 cP

@Shear Rate 1000 1/s,
Temperature 752 °F
Melt Viscosity; ASTM D3835
Solvay Specialty Polymers KetaSpire® KT-880 CF30 Polyetheretherketone (PEEK), 30% Carbon Fiber
KetaSpire® KT-880 CF30 is a high flow, 30% carbon fiber reinforced grade of polyetheretherketone (PEEK). Carbon-fiber reinforcement of KetaSpire® PEEK provides the maximum levels of mechanical..
Viscosity 450000 cP
450000 cP
A
Shin-Etsu Silicones LIMSâ„¢ KE2090-60AB Elastomer
KE-2090-60 is a selective self-adhesive liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is lo..
Viscosity 450000 cP

@Temperature 160 °C
450000 cP

@Temperature 320 °F
2.16 kg load; ISO 1133
EMS-Griltech Griltex® D 1357E Copolyester Hotmelt Adhesive (Apparel Interlinings)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Viscosity 450000 cP

@Temperature 160 °C
450000 cP

@Temperature 320 °F
2.16 kg load; ISO 1133
EMS-Griltech Griltex® D 1365E Copolyester Hotmelt Adhesive (Apparel Interlinings)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Viscosity 450000 cP

@Temperature 160 °C
450000 cP

@Temperature 320 °F
2.16 kg load; ISO 1133
EMS-Griltech Griltex® D 1365E Copolyester Hotmelt Adhesive (Technical Applications)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Viscosity 450000 cP

@Temperature 400 °C
450000 cP

@Temperature 752 °F
melt; ISO 11443
Victrex® PEEK 450GL15 Polyetheretherketone, 15% Glass Fibre Reinforced
Product Description:High performance thermoplastic material, 15% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, F..