Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

EMS-Griltech Griltex® D 1357E Copolyester Hotmelt Adhesive (Apparel Interlinings)

Category Polymer , Adhesive , Thermoplastic , Polyester, TP
Manufacturer EMS-Griltech
Trade Name Griltex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Griltech Griltex® D 1357E Copolyester Hotmelt Adhesive (Apparel Interlinings).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides for excellent resistance and dimensional stability of the finished garment. For technical applications, GRILTEX adhesive products are used to optimize the manufacturing process for the production of automotive interior components or parts for other applications. All values were determined on dried pellets.Main Application System: Paste DotMain Usage: Men's and Children's Wear, Women's Wear, Leisure and Sports Wear Data provided by EMS-Griltech.
Physical Properties Metric English Comments
Viscosity 450000 cP

@Temperature 160 °C
450000 cP

@Temperature 320 °F
2.16 kg load; ISO 1133
Melt Flow 23 g/10 min

@Load 2.16 kg,
Temperature 160 °C
23 g/10 min

@Load 4.76 lb,
Temperature 320 °F
cm<sup>3</sup>/10 min; ISO 1133
Thermal Properties Metric English Comments
Melting Point 110 - 115 °C
230 - 239 °F
DSC
Maximum Service Temperature, Air <= 60.0 °C
<= 140 °F
Laundering Resistance
Processing Properties Metric English Comments
Processing Temperature 120 - 140 °C
248 - 284 °F
Glue Line Temperature
Descriptive Properties Value Comments
Dry Cleaning Resistance Good
Steam Resistance Good