Material Notes:
KE-2090-60 is a selective self-adhesive liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is low enough to allow easy pumping through most injection molding systems.FeaturesSelective self adhesionNon adhesion to metalsInsert-molding and co-injection molding availableInformation Provided by Shin-Etsu Silicones of America, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
Viscosity 450000 cP
450000 cP
A
700000 cP
700000 cP
B
Linear Mold Shrinkage 0.022 cm/cm
0.022 in/in
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
Tensile Strength 7.30 MPa
1060 psi
Elongation at Yield 240 %
240 %
Tear Strength 36.0 kN/m
205 pli
Compression Set 9.0 %

@Temperature 200 °C,
Time 14400 sec
9.0 %

@Temperature 392 °F,
Time 4.00 hour
53 %

@Temperature 150 °C,
Time 3600 sec
53 %

@Temperature 302 °F,
Time 1.00 hour
Processing Properties Metric English Comments
Cure Time 10.0 min

@Temperature 120 °C
0.167 hour

@Temperature 248 °F
Press Cure
Descriptive Properties Value Comments
Appearance Translucent
Cure Rate 154
T90 (248°F, ODR)
94
T10 (248°F, ODR)