Zeon Chemicals Nipol® 1472X Nitrile Powder and Crumb Elastomer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Zeon Chemicals
Trade Name Nipol®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zeon Chemicals Nipol® 1472X Nitrile Powder and Crumb Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nipol 1472X is a copolymer of butadiene and acrylonitrile of medium-high acrylonitrile contnet modified to contain carboxyl groups. It contains sufficient antioxidant for normal storage conditions. Nipol 1472X shall be in the form of nominal 1/4" three-dimensional chips containing approximately 5% mineral dusting agent to prevent agglomeration. It shall be free from foreign material considered objectionable for normal applications.Carboxylated nitrile crumb, used in epoxy modification, for adhesives and composites. Contains talc partitioning agent.
Physical Properties Metric English Comments
Particle Size 9500 µm
9500 µm
Viscosity 100 - 1500 cP
100 - 1500 cP
Milled Cement; Zeon Test #1377
Mooney Viscosity 22 - 35

@Temperature 100 °C
22 - 35

@Temperature 212 °F
(1+4); Zeon Test #404
Ash 3.0 - 8.0 %
3.0 - 8.0 %
Zeon Test #873
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -31.0 °C
-23.8 °F
Descriptive Properties Value Comments
Bound ACN (%, acrylonitrile) 26-28
Carboxyl Content, % 0.07-0.08
Heat Loss (%) Max 0.5
Hot/Cold C