Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.000800 - 0.00500 cm/cm
0.000800 - 0.00500 in/in
Average value: 0.00373 cm/cm Grade Count:9
Overview of materials for Polycarbonate, Carbon + PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon + PTFE Filled". Each property range of values reported is minimum and maximum valu..
Linear Mold Shrinkage, Transverse 0.00300 - 0.00500 cm/cm
0.00300 - 0.00500 in/in
Average value: 0.00386 cm/cm Grade Count:7
Overview of materials for Polyetherimide (PEI), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu..
Linear Mold Shrinkage, Transverse 0.00100 - 0.00500 cm/cm
0.00100 - 0.00500 in/in
Average value: 0.00425 cm/cm Grade Count:12
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an..
Linear Mold Shrinkage, Transverse 0.00250 - 0.00500 cm/cm
0.00250 - 0.00500 in/in
Average value: 0.00387 cm/cm Grade Count:4
Overview of materials for Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler". Each property range of values reported is ..
Linear Mold Shrinkage, Transverse 0.00100 - 0.00500 cm/cm
0.00100 - 0.00500 in/in
Average value: 0.00300 cm/cm Grade Count:3
Overview of materials for Nylon 12, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of ..
Linear Mold Shrinkage, Transverse 0.000500 - 0.00500 cm/cm
0.000500 - 0.00500 in/in
Average value: 0.00188 cm/cm Grade Count:6
Overview of materials for Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced". Each property range of values reported is mi..
Linear Mold Shrinkage, Transverse 0.00300 - 0.00500 cm/cm
0.00300 - 0.00500 in/in
Average value: 0.00450 cm/cm Grade Count:4
Overview of materials for Polystyrene + Polyphenylene Ether, Glass Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Glass Filler". Each property range of values reported is minimum and ..