Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.000800 - 0.00500 cm/cm | 0.000800 - 0.00500 in/in | Average value: 0.00373 cm/cm Grade Count:9 |
Overview of materials for Polycarbonate, Carbon + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon + PTFE Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Linear Mold Shrinkage, Transverse | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | Average value: 0.00386 cm/cm Grade Count:7 |
Overview of materials for Polyetherimide (PEI), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Linear Mold Shrinkage, Transverse | 0.00100 - 0.00500 cm/cm | 0.00100 - 0.00500 in/in | Average value: 0.00425 cm/cm Grade Count:12 |
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an.. |
|||
Linear Mold Shrinkage, Transverse | 0.00250 - 0.00500 cm/cm | 0.00250 - 0.00500 in/in | Average value: 0.00387 cm/cm Grade Count:4 |
Overview of materials for Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler". Each property range of values reported is .. |
|||
Linear Mold Shrinkage, Transverse | 0.00100 - 0.00500 cm/cm | 0.00100 - 0.00500 in/in | Average value: 0.00300 cm/cm Grade Count:3 |
Overview of materials for Nylon 12, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Linear Mold Shrinkage, Transverse | 0.000500 - 0.00500 cm/cm | 0.000500 - 0.00500 in/in | Average value: 0.00188 cm/cm Grade Count:6 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced". Each property range of values reported is mi.. |
|||
Linear Mold Shrinkage, Transverse | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | Average value: 0.00450 cm/cm Grade Count:4 |
Overview of materials for Polystyrene + Polyphenylene Ether, Glass Filler This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Glass Filler". Each property range of values reported is minimum and .. |