Parker Chomerics CHO-SEAL® 6371 Conductive Elastomer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone
Manufacturer Parker Chomerics
Trade Name CHO-SEAL®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parker Chomerics CHO-SEAL® 6371 Conductive Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Good performance in moderately corrosive environments; material of choice for flange finishes needing “bite-through” for good electrical contact.Molded onlyRoHS Compliant Information provided by Chomerics
Physical Properties Metric English Comments
Specific Gravity 1.75 - 2.25 g/cc
1.75 - 2.25 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 55 - 75
55 - 75
ASTM D2240
Tensile Strength at Break >= 1.03 MPa
>= 150 psi
ASTM D412
Elongation at Break >= 100 %
>= 100 %
ASTM D412
Compression Set <= 40 %

@Temperature 100 °C,
Time 252000 sec
<= 40 %

@Temperature 212 °F,
Time 70.0 hour
ASTM D395 Method B
Thermal Properties Metric English Comments
Thermal Conductivity 1.10 W/m-K

@Pressure 2.07 MPa
7.63 BTU-in/hr-ft²-°F

@Pressure 300 psi
ASTM D5470
Maximum Service Temperature, Air 150 °C
302 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Flex TR10; ASTM D1329
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 0.10 ohm-cm
0.10 ohm-cm
without psa; CEPS-002
Shielding Effectiveness >= 100 dB
>= 100 dB
500 MHz (E Field); MIL-G-83528
>= 80 dB

@Frequency 2.00e+9 Hz
>= 80 dB

@Frequency 2.00e+9 Hz
CHO-TM-TP08
>= 80 dB

@Frequency 1.00e+9 Hz
>= 80 dB

@Frequency 1.00e+9 Hz
CHO-TM-TP08
>= 100 dB

@Frequency 1.00e+8 Hz
>= 100 dB

@Frequency 1.00e+8 Hz
CHO-TM-TP08
>= 100 dB

@Frequency 5.00e+8 Hz
>= 100 dB

@Frequency 5.00e+8 Hz
CHO-TM-TP08
Descriptive Properties Value Comments
Binder Silicone
Filler Ni/C
Heat Aging <0.25 ohm-cm
150°C for 48 hrs; CEPS-0002