Polymer Property : Specific Gravity = 1.42 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 1.36 - 1.42 g/cc
1.36 - 1.42 g/cc
ASTM D792
PolyOne Stat-Tech™ AT-CB2/000 CR Acetal (POM) Copolymer
Stat-Tech™ AT-CB2/000 CR XP020229R2Information provided by PolyOne
Specific Gravity 1.38 - 1.42 g/cc
1.38 - 1.42 g/cc
PEPL-10-W-21
Pearl Engineering PEPLPET D-101-SH Monofilament Resin
Used in the paper industry as paper pulp nets.
Specific Gravity 1.38 - 1.42 g/cc
1.38 - 1.42 g/cc
PEPL-10-W-21
Pearl Engineering PEPLPET FR-101-H Monofilament Resin
Used as textile grade flame retardant for furniture, car and plane upholstery.
Specific Gravity 1.38 - 1.42 g/cc
1.38 - 1.42 g/cc
PEPL-10-W-21
Pearl Engineering PEPLPET B101H Monofilament Resin
Generally used in monofilament v-belts, zips and other technical applications.
Specific Gravity 1.36 - 1.42 g/cc
1.36 - 1.42 g/cc
ASTM D 792
Karina 802-06/795-CRM Blue PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.36 - 1.42 g/cc
1.36 - 1.42 g/cc
ASTM D 792
Karina 837-35/1-A-ERYB-LMP Ivory PVC Compound
Heavy metal free PVC compound recommended for extrusion of furniture profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.36 - 1.42 g/cc
1.36 - 1.42 g/cc
ASTM D 792
Karina 937-48/1-CY-IS-BZ Black PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.36 - 1.42 g/cc
1.36 - 1.42 g/cc
NBR NM-IEC 60811-1-3
Karina E 18/89-FC-LMP Gray Color Concentrate for PVC
Color concentrate recommended for application in PVC compounds for electrical wires and cables. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes.Important con..
Specific Gravity 1.36 - 1.42 g/cc
1.36 - 1.42 g/cc
ASTM D 792
Karina E 845-35/2-CRM Ivory PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.401 - 1.42 g/cc
1.401 - 1.42 g/cc
Dow UVI-6976 Photoinitiator
UVI-6976 is a cationic photoinitiator containing a mixture of triarylsulfonium hexafluoroantimonate salts in propylene carbonate. UVI-6976 photoinitiator is used to UV-cure CYRACURE™ cycloaliphati..
Specific Gravity 1.38 - 1.42 g/cc
1.38 - 1.42 g/cc
ASTM D792
Compuestos Dominicanos Polycom AK-050380 PVC
Description: Compuestos Dominicanos, S.A. manufactures PVC compounds for the production of high quality electrical wire and cable with excellent insulation properties and smooth finish. Polycom prod..
Specific Gravity 1.38 - 1.42 g/cc
1.38 - 1.42 g/cc
ASTM D792
Compuestos Dominicanos Polycom AK-051090 PVC Compound
Compuestos Dominicanos, S.A. manufactures high quality covering PVC for the production of electrical wire and cable providing excellent insulation properties and smooth finish. Their products are d..
Specific Gravity 1.38 - 1.42 g/cc
1.38 - 1.42 g/cc
ASTM D-792
Axiall 1131-57D Wire & Cable Flexible PVC
Non-lead stabilized 105°C rated jacket compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Specific Gravity 1.38 - 1.42 g/cc
1.38 - 1.42 g/cc
ASTM D-792
Axiall 12792 Wire & Cable Flexible PVC
General purpose, 75°C rated non-lead stabilized jacket compound with good low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Specific Gravity 1.38 - 1.42 g/cc
1.38 - 1.42 g/cc
ASTM D-792
Axiall 12802 Wire & Cable Flexible PVC
Non-lead stabilized general purpose jacket recommended for 75C applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Specific Gravity 1.38 - 1.42 g/cc
1.38 - 1.42 g/cc
ASTM D-792
Axiall 14890 Wire & Cable Flexible PVC
General purpose UL approved 720 hour sunlight resistant jacket suitable for a maximum 80°C temperature rating at a 1/32" wall. Recommended for UF-B and NM-B constructions and also RG59 coaxial cab..
Specific Gravity 1.38 - 1.42 g/cc
1.38 - 1.42 g/cc
ASTM D-792
Axiall 16902 Wire & Cable Flexible PVC
Non-lead stabilized, 90°C rated fiber optic riser jacket.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Specific Gravity 1.38 - 1.42 g/cc
1.38 - 1.42 g/cc
ASTM D-792
Axiall 17870 Wire & Cable Flexible PVC
TW, THW insulation compound. Oil II rated. 720 hour sunlight resistant in all colors.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Specific Gravity 1.38 - 1.42 g/cc
1.38 - 1.42 g/cc
ASTM D-792
Axiall 22902 Coax & Telecom Flexible PVC
Non-lead stabilized riser jacket recommended over PVC and FRHDPE primaries. Maximum service temperature rating of 75°C.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in..
Specific Gravity 1.38 - 1.42 g/cc
1.38 - 1.42 g/cc
ASTM D-792
Axiall 38951 Wire & Cable Flexible PVC
Low cost AWM jacket for SPT, SVT, SJT applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Specific Gravity 1.38 - 1.42 g/cc
1.38 - 1.42 g/cc
ASTM D-792
Axiall 8758 Moldings & Extrusions Flexible PVC
A general purpose extrusion compound recommended for extruded shapes, weatherstrips and flexible gaskets. Formulated for good UV light resistance and low temperature properties.Information provided..
Specific Gravity 1.38 - 1.42 g/cc
1.38 - 1.42 g/cc
ASTM D-792
Axiall 8850 Moldings & Extrusions Flexible PVC
General purpose extrusion.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Specific Gravity 1.38 - 1.42 g/cc
1.38 - 1.42 g/cc
ASTM D-792
Axiall 8880 Moldings & Extrusions Flexible PVC
General purpose non-lead stabilized extrusion compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Specific Gravity 1.38 - 1.42 g/cc
1.38 - 1.42 g/cc
ASTM D-792
Axiall 8910 Moldings & Extrusions Flexible PVC
Extrusion compound especially formulated for extruded T-moldings, tubings, and other shapes where uniform flow through the die is required.Information provided by Georgia GulfGeorgia Gulf became Axi..
Specific Gravity 1.38 - 1.42 g/cc
1.38 - 1.42 g/cc
ASTM D-792
Axiall EX1063 Coax & Telecom Flexible PVC
Non-lead stabilized, fiber optic compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Specific Gravity 1.38 - 1.42 g/cc
1.38 - 1.42 g/cc
ASTM D-792
Axiall 12791 Wire & Cable Flexible PVC
General purpose, 75°C rated non-lead stabilized jacket compound with good low temperature properties and 720 hour sunlight resistance.Information provided by Georgia GulfGeorgia Gulf became Axiall ..
Specific Gravity 1.38 - 1.42 g/cc
1.38 - 1.42 g/cc
ASTM D-792
Axiall 1055 Wire & Cable Flexible PVC
NM-B and UF-B jacket with good low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Specific Gravity 1.38 - 1.42 g/cc
1.38 - 1.42 g/cc
ASTM D-792
Axiall 4750 Flexible PVC
General purpose molding and extrusion compound well suited for automotive floor mats.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Specific Gravity 1.36 - 1.42 g/cc
1.36 - 1.42 g/cc
ASTM D 792
Karina 837-10/37-A-ERYB-LMP White PVC Compound
Heavy metal free PVC compound recommended for extrusion of furniture profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.38 - 1.42 g/cc
1.38 - 1.42 g/cc
ASTM D792
Compuestos Dominicanos Polycom AU-050695 PVC Compound
Compuestos Dominicanos, S.A. manufactures high quality covering PVC for the production of electrical wire and cable providing excellent insulation properties and smooth finish. Their products are d..