Material Notes:
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.36 - 1.42 g/cc
1.36 - 1.42 g/cc
ASTM D 792
ASTM Color -1.16 - 1.84
-1.16 - 1.84
Color A, ME 12
3.43 - 6.43
3.43 - 6.43
Color B, ME 12
90.4 - 93.4
90.4 - 93.4
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore D 78 - 82

@Time 15.0 sec
78 - 82

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 34.3 MPa
>= 4980 psi
ASTM D 638
Descriptive Properties Value Comments
Application Fittings