Material Notes:
General purpose extrusion.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.38 - 1.42 g/cc
1.38 - 1.42 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 82 - 88
82 - 88
delayed; ASTM D-2240
Tensile Strength, Yield 17.6 MPa
2550 psi
ASTM D-638
Elongation at Yield 340 %
340 %
ASTM D-638
100% Modulus 0.0110 GPa
1.60 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -23.0 °C
-9.40 °F
ASTM D-746
Processing Properties Metric English Comments
Melt Temperature 179 °C
355 °F