Material Notes:
Non-lead stabilized, 90°C rated fiber optic riser jacket.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.38 - 1.42 g/cc
1.38 - 1.42 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 87 - 93
87 - 93
delayed; ASTM D-2240
Tensile Strength, Yield 17.2 MPa
2500 psi
ASTM D-638
Elongation at Yield 222.7 %
222.7 %
Air Aging: 168 hours @ 121°C; 30 mil slabs; UL 1581
290 %
290 %
ASTM D-638
100% Modulus 0.01217 GPa
1.765 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -27.0 °C
-16.6 °F
ASTM D-746
Oxygen Index 30 %
30 %
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 188 °C
370 °F