Dow UVI-6976 Photoinitiator

Category Polymer , Thermoset , Epoxy
Manufacturer Dow Chemical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow UVI-6976 Photoinitiator.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
UVI-6976 is a cationic photoinitiator containing a mixture of triarylsulfonium hexafluoroantimonate salts in propylene carbonate. UVI-6976 photoinitiator is used to UV-cure CYRACURE™ cycloaliphatic epoxide resins, vinyl ethers and other cationically curing materials.Information provided by Dow
Physical Properties Metric English Comments
Specific Gravity 1.401 - 1.42 g/cc
1.401 - 1.42 g/cc
Maximum Moisture Content 1.0
1.0
wt% water
Optical Properties Metric English Comments
Gardner Color Number <= 7.0
<= 7.0
Descriptive Properties Value Comments
Hydroxyl Number mg KOH/g 187