Teknor Apex Sinvicomp SIM 5515 Polyvinyl Chloride, Flexible

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Flexible Grade
Manufacturer Teknor Apex Company
Trade Name Sinvicomp
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Sinvicomp SIM 5515 Polyvinyl Chloride, Flexible.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: Asia Pacific Features: High Strength Uses: Electrical/Electronic Applications < Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.35 g/cc
1.35 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
ASTM D2240
Tensile Strength, Yield 10.80 MPa
1566 psi
Change in tensile strength after 168 hours at 212°F; ASTM D638
12.0 MPa
1740 psi
9.8 in/min; ASTM D638
Elongation at Break 152 %
152 %
Change after 168 hours at 212°F; ASTM D638
190 %
190 %
9.8 in/min; ASTM D638
Electrical Properties Metric English Comments
Volume Resistivity 5.00e+13 ohm-cm

@Temperature 20.0 °C
5.00e+13 ohm-cm

@Temperature 68.0 °F
BS 2782