Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Teknor Apex APEX® SRP 2700A Polyvinyl Chloride, Rigid

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Rigid Grade
Manufacturer Teknor Apex Company
Trade Name APEX®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex APEX® SRP 2700A Polyvinyl Chloride, Rigid.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Forms: Pellets Additional Information: HDT, Annealed; 24 hours, 156°FInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.35 g/cc
1.35 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 77
77
10 seconds; ASTM D2240
Tensile Strength at Break 46.8 MPa
6790 psi
ASTM D638
Elongation at Break 120 %
120 %
ASTM D638
Tensile Modulus 2.35 GPa
341 ksi
ASTM D638
Flexural Modulus 2.68 GPa
389 ksi
ASTM D790
Izod Impact, Notched 2.03 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
3.80 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
Compression Molded; ASTM D256
Dart Drop Total Energy 111 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
0.208 ft-lb/mil

@Thickness 0.125 in,
Temperature 73.0 °F
Procedure B, 0.125" Conical Dart
Thermal Properties Metric English Comments
Vicat Softening Point 76.7 °C
170 °F
ASTM D638
Descriptive Properties Value Comments
Appearance Opaque
Copyright © lookpolymers.com All Rights Reserved