Parker Chomerics CHO-SHIELD® 4900 Conductive Coating

Category Polymer , Adhesive , Thermoset
Manufacturer Parker Chomerics
Trade Name CHO-SHIELD®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parker Chomerics CHO-SHIELD® 4900 Conductive Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CHO-SHIELD® 4900 silver-filled acrylic coating provides the highest levels of EMI shielding, as well as anti-static protection and grounding surfaces. It offers convenient fast tack and drying. Filler systems include nickel, silver, silver-copper, or nickel-silver blends. Information provided by Chomerics
Physical Properties Metric English Comments
Specific Gravity 1.35 - 1.65 g/cc
1.35 - 1.65 g/cc
Volatile Organic Compounds (VOC) Content 731 g/l
731 g/l
Bulk
Thickness 25.4 microns
1.00 mil
Recommended
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 93.0 °C
199 °F
Minimum Service Temperature, Air -54.0 °C
-65.2 °F
Electrical Properties Metric English Comments
Surface Resistivity per Square <= 0.050 ohm
<= 0.050 ohm
Processing Properties Metric English Comments
Cure Time 1440 min

@Temperature 23.0 °C
24.0 hour

@Temperature 73.4 °F
Shelf Life 6.00 Month
6.00 Month
Spray
9.00 Month
9.00 Month
Bulk
Descriptive Properties Value Comments
Binder Acrylic
Consistency Thin Fluid
Coverage 34 ft2/lb
Filler Ag
Mix Ratio 1-part
Spraying Viscosity, #2 Zahn Cup 19 - 22 sec
Users viewing this material also viewed the following: